beading bloke

Hi all.
        My bottle of bead release has gone a bit thick and lumpy despite giving it a good shake before using it.can i just add water to it to make it OK again.May thanks.

Tollgate-Debs

I add water when needed - a little at a time and mix it well.  I also add a few beads into each pot which helps to agitate the mixture when shaken.

Debs

Lush!

Just make very very very sure you've put the lid on properly before you shake!  ;)


www.lushlampwork.etsy.com

GoodMonkey

Quote from: Lush! on November 24, 2009, 07:29:41 PM
Just make very very very sure you've put the lid on properly before you shake!  ;)

There speaks the voice of experience.......

julieHB

Quote from: GoodMonkey on November 24, 2009, 08:06:10 PM
Quote from: Lush! on November 24, 2009, 07:29:41 PM
Just make very very very sure you've put the lid on properly before you shake!  ;)

There speaks the voice of experience.......

...erm...I don't shake the bottle any more - I use a thick mandrel and stir it before use....I never, never, ever want to clean up splattered bead release from all over my glass, floor, workbench ever again!!!  ::)
Julie xx

                           My Webbie - My Flickr

Margram

I've written a warning on my lid - it's only a matter of time before I get so used
to seeing that that I just don't see it... ::)

Someone (was it Trudi?) said to use distilled water to dilute it.
Marg x  Etsy Flickr My blog

Steampunkglass

Someone posted it's better to use distilled water; I've only been using tap water and the mix isn't as good as when I bought it so may well help prolong the life of it.

fionaess

I've always used tap water with my Foster Fire - and its fine...just as good as the first time :)


If it's got a hole, it's a bead !

sublimekate

Yep I just put some tap water in, and if it's too runny leave the lid off for a bit  ;D

Shaking it with the lid off!! Oh dear, messy  ;D

Les

Quote from: Lush! on November 24, 2009, 07:29:41 PM
Just make very very very sure you've put the lid on properly before you shake!  ;)

Damn right ! ;)

Betty the Chook

I use a little whisk to give it a good mix up. Just don't leave the whisk in as it goes rusty very quickly - not nice.... but better than bead release splattered everywhere!
I'm really a Fiona, not a Betty the Chook.
It's just that I rather like hens
.... more than a bit actually

http://www.rhinoglassbeads.com

glassworks

the only thing to be aware of is NOT TO USE SOFTENED WATER!!!!.... apparently the salts cause the fosterfire to breakdown and crumble when dry?.. i asked robin about this and she confirmed it is best to use distilled or plain tap water only!...

and, tighten the lid... i've done it too.... i also chuck a few fuggly beads into the bottle to act as a "stirrer" to get the lumps off the bottom.. makes a neat rattle too!...

princess pink

i've been using bottled mineral water as i didnt have any distilled...do you think thats ok?

turnedlight

I've been using rainwater - just leave my jars outside the shed - I wonder if that's bad? ??? :)
kathryn

glassworks

rain water is fine... i would think that bottled (flat) water is fine too, as it is mostly just filtered tap water anyway!..  ;D :D ;D

seriously though, from what robin explained it was the additional salts that the water softener added that caused the issues...

anyone else had any experience of the flaky bead release - i know we replaced a few bottles before robin cottoned on to what the issue was...