tack fuse

Started by handmadeheaven.biz, February 27, 2007, 11:13:03 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

handmadeheaven.biz

does anyone have any tack fuse schedules for bullseye? i have lots of full and slump fuse ones but none for tacking.

help!

SilverClay

#1
Hi Helen,

Have you checked the Bullseye Tech Notes - they are great, has all the info you could ask for.

Think this is the one who gives the tack fuse details.
www.bullseyeglass.com/pdfs/technotes_tipsheets/TechNotes_04.pdf

Petra
Art Clay Senior Instructor



edited to replace weblink - see below



BeadyBugs

Sorry Steph I haven't - I've been meaning to have a play with tack fusing, but not got round to it yet.  It's on my ever expanding list of things to do. ;D  I've got to make a beady zoo now...I might be some time!  LOL! ;D

And hi Petra!  Lovely to see you here. :D

HP x
Helen P

SilverClay

#3
Hello Helen - thanks for the hi!

And Steph, sorry for calling you Helen!!  ::) Duh. I think it was because I had just been looking at Helen's zebra - ooooooh, he's adorable...

Petra
Art Clay Senior Instructor


edited to replace weblink - see below

handmadeheaven.biz

not a problem Petra. I've had worse!

HP - I think Beck might have something.... :)

BeadyBugs

Hehehe!  Thanks Petra. :D

Oh fab Steph - you'll have to let us know how you get on. ;D

HP x
Helen P

handmadeheaven.biz

it's for that interior design shop but i have a sneaky feeling it won't work. i DO need a tack fuse schedule tho. been wanting to give it a go myself for ages & thought i had one.

Pam

Hi Steph, I dont know whether this is any help to you but I have just finished some 30cm x 10cm panels in a textured design (tack fused i guess you may call it). They have come out just perfect, rounded edges, strong texture, all pieces have slumped over each other nicely. I used your full fuse schedule but dropped the top temperature to 730 degrees centigrade (held for 10 mins).
Pam

handmadeheaven.biz

as far as i can gather pam, that's the way you do it. keep the same schedule for full fuse but reduce that top temperature :)

ps: got photos of these pieces? ;)

Pam

I'LL post them tonight when I am back from work.

Les

OOOoohhhhh yummy !!!! I love tack fused stuff...... it's so very tactile !!!

Pam

As promised. What do you think?

♥♥Tan♥♥

That is gorgeous Pam, I have some pictures of my newbie tack fusing that I must post in my diary link but youve kind of put me to shame now with your lovliness :-[

handmadeheaven.biz

oo, they're lovely pam. i particularly like the bottom one. how are you going to display them?

Pam

Well, I have lots of ideas but the easiest (for me that is ) was to put them in a block of wood. Hubby bought some 4 inch whoops 10cm oak, routered it and put a slit in the middle for thme to stand in. Looks quite classy.