encasing a pressed bead?

Started by bubblefizz, March 10, 2009, 12:50:48 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

bubblefizz

can you tell me how you encase a pressed bead, do u make the core the width of the press, or do you make a barrel shape  ???
what way do u do it? its doing my head in, i end up with the core all mushed up, its awful
so im thinking there has to be a technique for this!

hollergrafik

I have pressed the bead in a smaller sized press first, encased then press in a bigger one, HTH's

theflyingbedstead

It sounds like you are heating your core too much - try just keeping it warm at the back of the flame whilst you encase.
I tend to press my beads after they have been encased.
I hope this helps!
Charlotte x

bubblefizz

Quote from: hollergrafik on March 10, 2009, 12:53:22 PM
I have pressed the bead in a smaller sized press first, encased then press in a bigger one, HTH's

ohh shall try this  ;D thank you!