Katiequiggle

Ok silly question from a not so new newbie but, Please someone tell me, what do you do with shards.  I have some that someone sent me a while ago and I havn't used them yet as I'm not sure what to do with them.

Stacy

I'm no expert I think I have played with 4 or 5 beads with shards in all...

Basically I make a base bead, hold the shard with a pair of twesers (sp?) and then waft it in the top of the flame to get it warm, then I kind of just touch it to the bead so it sticks, (a bit like silver wire) and then I let it fall where it wants to, I like the way it gives a material effect.


Chelly77

I was wondering that too :)  and now I know ;D

saffie

first time i used them i just blasted them with heat they shrink loads!!!  ;) Now i do what Stacy just said and they keep their size more!!

Jolene

There is a nice section in the wiki about making and using shards

http://www.frit-happens.co.uk/wiki/Shards

Katiequiggle


June

Maybe we could have a 'Shards Show & Tell' thread? 

Katiequiggle


June

Just need somebody that has a picture of bead or two using shards now  ;)  Anybody?

fionaess

Here you go.. sorry they are late, but I just noticed this thread...
  silver ivory shared melted in

  melted in again

  shards laid over the top


If it's got a hole, it's a bead !

June

Oooo, lovely, Fiona, particularly love the middle set.  Thanks !  ;D

Kaz

These were all done with shards from Jo

With the last 2 I melted silver leaf over the top to get the antique-y effect.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

paterperlo

Sorry not mine...
from my wife Aleksandra. Selfmade shards and handpulled murrini.


Matthias

Kaz

Jo's silvered hades shards over dirty martini with more silver foil applied and tiny hades bumps

Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Black Heart Beads

Some great examples but this one is stunning

Quote from: paterperlo on March 04, 2009, 10:33:59 PM
Sorry not mine...
from my wife Aleksandra. Selfmade shards and handpulled murrini.