Making a ring?

Started by lemon kitten, January 19, 2009, 03:54:22 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

lemon kitten

I've been asked to make a ring for someone...and I have'nt a clue how to go about it?? does anyone have any tips or ideas as to how to make a nice ring??  I don't really want to make it using a ring mandrel as that will govern the sizing somewhat, I do have a few metal ring mounts, and one that I guess I could make round beads on and wire onto it....any other suggestions??

janey x
Never stand up in a canoe!

Billie

Have you got the current issue of Beads and Beyond?  There's a wire wrap ring step by step design in there you could use to mount a bead on.

mizgeorge

Would something like this work Janey?



I can happily write you a quick tute if you like



bluefairy

They are BOOTIFUL, please do a tute George!!  ::)
Helen xx

My Etsy     My Facebook     My Folksy

Billie

*Jumping up and down*  Yes!!  Like that!!  George, yours are GORGEOUS!!  Would you do a tute?  I'd love to be able to do one (or can I commission you in exchange for beadies?)

dinah46


SMHBuss


Chameleon


June

Very clever, George, those rings are lovely  ;D

mizgeorge

Quote from: SMHBuss on January 19, 2009, 04:44:34 PM
Are those adjustable??

Sadly not very adjustable (there's a bit of 'give' but that's it). I end up making a  range of sizes - but they take literally a couple of minutes so can be done on the spot if needed.

ebj

Those rings are beautiful!!

You could make a pure silver ring from art clay silver :)
Emma

Art Clay Senior Instructor & Lampworker

www.emmabaird.wordpress.com

SMHBuss

They are lovely.  I do some similiar but not as nice as your I'm afraid!

Vicki

they are gorgeous George  ;D  I hate seeing rings on here, because I love them & can't wear them  :'(

Bumpy Beads

George those are really impressive! But what is even more impressive is that you can make one on the spot!

Heather


My Etsy Shop

lemon kitten

Those are gorgeous!!!  I'd LOVE you to write me a TUT if you don't mind!  I will also get the Beads and Beyond issue mentioned here.  Once again thanks for all your great help.

Janey x
Never stand up in a canoe!