Things you can do with frit

Started by Jolene, July 11, 2008, 12:16:19 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.


afina

You can also make easy twisties or latticino-cane with frit.

You need:
* any pale opaque color (for twisty) or clear (for latticino-cane)
* fritblend of choice
* a rod of clear.

How to make the cane:
1) Melt a big blob
2) roll blob in fritblend
3) melt in completely
4) encase in clear
5) reheat the blob, pull and twist.
Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at

Jolene

That sounds fun, I am gonna try this next time I get near my torch ;D

Great tip Verena

Katerina


turnedlight

Wow - I'm going to try that too! Thanks :)
kathryn