sugary beads

Started by turquoise, July 02, 2008, 05:53:24 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

turquoise

Hi , can anyone tell me how you make those sugary looking beads that people seem to be doing at the mo, I really like the look of these and fancy having a go?


www.morellobeads.co.uk

beads-on-toast

it's all about the frit mate

clear frit - Beadysam stocks it

Kaz

Lead crystal 0 or 00
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Katerina

Quote from: Kaz on July 02, 2008, 06:25:28 PM
Lead crystal 0 or 00
Kaz
which one is smaller? 0 or 00?

Kaz

00 is very fine - like powder almost.
You have to be careful when you have applied it to waft it in and out of the flame high up and quite gently as it can 'catch' like sugar and will discolour.
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Pandanimal

I love the sugared beads too.
They look so good and textural.

So I've just ordered some frit from beadysam.
I bought the one she had listed for sugaring beads with. An 80grm pot of it, I think that might be enough to practise with.
I bought some other stuff as well. Just couldn't help myself!

Katerina

thank you Kaz well I was on this website and bought example park last night. FNF but couldn't find this sugar one....

Katiequiggle

Oooh sugary beads sound lovely, wheres a picture please.

Kaz

This will give you an idea

Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Katiequiggle

OOOh yummy, I'm having some of that. ;D

beads-on-toast


turquoise

oh cricky the more I see them the more I like these sugary beads.


www.morellobeads.co.uk

beadysam

Clear frit is my most popular item at the moment for some reason..... ;) ;D

Katerina

Quote from: beadysam on July 03, 2008, 08:34:37 PM
Clear frit is my most popular item at the moment for some reason..... ;) ;D

beadysam I made an order last night...(FNF collection and some more) but couldn't find clear one. Any help? 

turquoise

me too I could not see the clear one anywhere!


www.morellobeads.co.uk