how do you get you round beads all the same size?

Started by turquoise, June 16, 2008, 07:00:23 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

turquoise

HI just wondering how people know when you have enough glass on the mandrel to make all of your tyre shaped beads and round beads?

I am making sets and am struggling to get all beads exactly the same size.

;) ;D


www.morellobeads.co.uk

dangerousbead

It's practice sadly. Try making more than one on a mandrel and matching it up  to the other. When you've made about 3 gazillion you'll be an expert, i'm up to about 100 & still nothing is the same as the last.  >:(

misspixie

Um... Nope. Still not entirely there - well, not if you want them a reasonable size anyway! I can either do tiny and matching, or huge and matching, nothing in between...

flowerjasper

i dont!!
as dangerous says( i would love o be known as dangerous!)
PPP,
i made a set today,( i use the word set in its widest form),

few, if any of the beads matched, am going to plug the abstact/ bispoke angle i think!!
x

Les

What I used to do when I was first starting to make sets, was to make one plain bead at the size I wanted on a mandrel and keep it at my table, so I could compare all subsequent beads to it as I went along.

HTH

xxx

Kaz

Quote from: Les on June 17, 2008, 07:02:08 AM
What I used to do when I was first starting to make sets, was to make one plain bead at the size I wanted on a mandrel and keep it at my table, so I could compare all subsequent beads to it as I went along.

HTH

xxx
Obvious - but brilliant!!! Thanks Les.
I guess the only thing to remember is that the glass does expand when it's hot and then shrinks back a bit so you have to factor that in.
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Les

Having said that though.... my bead sets are never exactly the same size.... but hey... they're handmade... it's to be expected.

The one thing I'll never attain (thankfully) is factory produced precision ;D ;D

xxx

Lush!

Great suggestion Les!

I rarely have any luck making more than one bead on a mandrel. I need to be able to keep my eye on one bead at a time ... maybe that's cos my other eye is watching the DVD player!!  ;D ;D ;D



www.lushlampwork.etsy.com

Mary

Graduated sets are good! And I always make more beads than I need, and pick the best match.

Pat from Canvey

I use a six in one marble and bead mold if I need to turn out spherical beads the same size. Rotate the bead in the mold to get a spherical shape. you can also use them to get an oval shape by using the mold size larger than the bead you want and rotating off centre. Martin sells graphite marble paddles. You can also use the paddles to help with implosion pendants.

turquoise

super dooper, thanks for all of that advice I reckon I will try the bead on the table trick next time.

Or just make graduated sets!!!! :D ;)


www.morellobeads.co.uk

Josephine

I've got a mark on the side of my marver. Can't say they are always identical but they are within 1mm of eachother. Lots of practice really.

dangerousbead

Quote from: flowerjasper on June 16, 2008, 11:35:13 PM
i dont!!
as dangerous says( i would love o be known as dangerous!)
PPP,
i made a set today,( i use the word set in its widest form),

few, if any of the beads matched, am going to plug the abstact/ bispoke angle i think!!
x
Ha Ha you wouldn't!  I get burnt a lot he he