Soldering a jump ring

Started by Dee Dee, May 29, 2008, 02:50:14 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Dee Dee

Hey everyone, hope you are having a good day.

I have a small problem, I have made a necklace with seed beads and a paua shell pendant, but the oval jump ring attaching the pendant came slightly apart allowing the pendant to drop off the necklace.  Annoyingly this happened 2 hours after my customer bought it!  See picture. 

Is there a way to join the jump ring, so that it doesn't happen.  I have tried to solder it (on a test piece), without the necklace attached, but the shell burns, no matter how careful I am.  Any thoughts, anyone???


,

turnedlight

Can you fit a heavier bit of wire through? If it's hard and heavier weight, (you can tap it with a mallet to harden, or even hammer the wire so it's slightly flatter and make it back into a jump ring) it shouldn't pull apart..
kathryn

julieHB

Hi, have you considered using something else than a jump ring? 

Here I have used beading wire with seed beads, crimped twice at the back:


Good luck!
Julie xx

                           My Webbie - My Flickr

Kaz

#3
Why not just use pre-soldered jump rings for the bit that connects to the necklace ends and then open jump rings to attach the clasp onto that?
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Pat from Canvey

It might be possible to shield the shell with fibre blanket whilst soldering the silver but I've not tried it. Are you using a small torch  with a pencil flame to solder. Just been away and tried a solder without any shielding. The picture is at
http://pic20.picturetrail.com/VOL1426/5604171/12685369/319218851.jpg
The soldered area is at about 10.00 in the picture. I already had some paua shell pre-drilled and some silver jump rings made. There isI think a small area of burn under the solder, but thats because of the shape of the shell and the circular jump ring being so close. If I was doing this for real, I'd use an oblong jump ring to get the site to be soldered as far away as possible from the shell. This would also help with a bit of shielding.
Alternatively you could use a wrapped loop construction that would not need to be soldered.
The torch I used was a Microflame Piezo Instant Ignition Pencil Flame Torch which runs on gas lighter refills.

DragonflyLynne

If you use as thick a jump ring as will fit, and close it so the 2 edges are pushing against each other with no visible gap it should be fine. I have a large piece of yellow turquoise, front drilled like your pendant, that is attached with one ring and it is absolutely fine. I wear it a lot. Let me know what size you would like and I'll send you one.  ;D


for chain maille supplies, kits & workshops, bespoke headpins, earwires and more! Meddle ye not in the affairs of dragons, for you are crispy and taste good with ketchup! Dragonfly (Lynne)

Dee Dee

Thanks guys, I think I have some very thick jump rings.......somewhere!
Thanks for trying Pat, it is a small torch I was using, but don't want to try it again as I only have one of these pendant's left!

I might try Julie's idea, is that one piece of jewellery wire wrapped round twice, or two separate loops?

Is there any reason why a soldering iron wouldn't work, rather than a torch?



julieHB

Quote from: Dee Dee on May 30, 2008, 01:23:41 AM
Thanks guys, I think I have some very thick jump rings.......somewhere!
Thanks for trying Pat, it is a small torch I was using, but don't want to try it again as I only have one of these pendant's left!

I might try Julie's idea, is that one piece of jewellery wire wrapped round twice, or two separate loops?

Is there any reason why a soldering iron wouldn't work, rather than a torch?

Int the picture I showed it is bendalon wire wrapped around twice, with 2 crimps at the back.

You use a soldering iron with electric components and soldering tin....I think you need higher temperatures for sterling silver and silver solder, hence a torch (please correct me anyone if I am wrong).
Julie xx

                           My Webbie - My Flickr

Pat from Canvey

You also use a higher wattage (100-200 watts) solering iron to make copperfoil and stained glass lead panels, hence my avatar on the left. It's a lamp composed of hexagons and pentagons soldered together with a ceramic base I also made.

LittleHen

Quote from: Pat from Canvey on May 30, 2008, 08:44:13 AM
You also use a higher wattage (100-200 watts) solering iron to make copperfoil and stained glass lead panels, hence my avatar on the left. It's a lamp composed of hexagons and pentagons soldered together with a ceramic base I also made.
When I did stained glass I also used to make these shapes it's the same as a football and Carbon 60 - an interesting allotrope of carbon also called Buckminsterfullerene!! I'm a sad ex-chemist  :D ;D :D
I never made a lamp though, do you have a link to a bigger piccie?
Jessie  ;)

Pat from Canvey

Jessie
Have a look at http://www.uniqueglass.co.uk/lampshades.htm and scroll down to the bottom right of the page. Click on the thumbnail for a bigger picture. The website is my old one which still uploads despite me telling them I'd retired and wasn't paying anymore. I was keeping the web address though. I still have all my "stuff" and use some of my stained glass for beadmaking.
As for sad ex-chemist, one of my sons is an analytical chemist testing water quality for Southern Water.

Dee Dee

Thanks for your help guys, I went Julie's seed bead route, and it looks good.  Sometimes you just can't see the wood for the trees!!!

STEPH

Yellow friend

On another occasion you could try putting the pendant under cold water whilst soldering.  Make sure the joint is clean and a close fit,you can buy a flux & solder paste in a syringe (Cooksons) which I find invaluable for awkward jobs.  Heat with a cooks torch and remove the heat as soon as it starts to flow (takes a few seconds), that way you don't get too much black stuff to remove.  Use a silver cloth to polish.  You can also buy a heat resistant paste to smother the piece you don't want heating up but its not that easy to use.

Hope it helps.

Shelia
www.crocosmiajewellery.com
www.crocosmiajewellery.etsy.com

Dee Dee

Quote from: Yellow friend on August 08, 2008, 04:42:40 PM
On another occasion you could try putting the pendant under cold water whilst soldering.  Make sure the joint is clean and a close fit,you can buy a flux & solder paste in a syringe (Cooksons) which I find invaluable for awkward jobs.  Heat with a cooks torch and remove the heat as soon as it starts to flow (takes a few seconds), that way you don't get too much black stuff to remove.  Use a silver cloth to polish.  You can also buy a heat resistant paste to smother the piece you don't want heating up but its not that easy to use.

Hope it helps.

Shelia

Apologies Sheila, I've only just spotted your reply to my post.  I will look into that flux & solder paste in a syringe, sounds good.

Thanks for your advice.

Steph


Yellow friend

It is excellent stuff, bit expensive but it lasts for ages.  Smothering the bead in paste called Warmestop (German I think) helps prevent it cracking, bit messy but it does work.

Hope it helps

Shelia
www.crocosmiajewellery.com
www.crocosmiajewellery.etsy.com