Main Menu

gallery archive 08

Started by beads-on-toast, January 01, 2008, 11:13:04 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Paula

#180
Day two. I had about an hour and a half to play today, and I'm fairly pleased with them. I'm feeling more like the glass is my friend rather than my enemy!

Paula

Diane

Lovely beads going on here - those flowers are beautiful.
I have done a few new sets this week.
[img= 400 width]http://[/img]
[img= 450 width]http://[/img]

glassworks

my first boro marble - playing with implosions and fuming, keeping it really simple so only blue and clear...







be gentle.....  ;D ;D

Diane

Absolutely stunning beads Dora. A set from me just finished
[img= 500 width]http://[/img]
Diane

Katiequiggle

#184
Fab second go beads Paula, great shapes, no pointy bits like mine were are still are sometimes  ;D

I've had a whole school hours day in the shed today before I had to go to school to see 'THE' video.  I made these.  I'm loving the colours, the yellowy looking long ones are actually ivory.




turnedlight

Wow! Diane, those colours are gorgeous! And Les, that top one is beautiful and arty :)
I've been practising discs, as people keep asking me to do cufflinks, but I find it really hard to get a disc even, and then to do another, matching one.. well! PPP tomorrow!

         
       
         

and some more nuggety ones..

         
kathryn

Dreams of Glass

OMG some stunning work here, I've missed show and tell, in fact I've missed you all.

Here are two Gothic Fairies I did before Towcester, I don't have anything new to show at the mo as working on my swops  :)


Ingrid                         
xx

ebj

Stunning work from everyone :O  Beautiful beads. I just LOVE those little fairies, they are just adorable! I'm really inspired by this thread :) 

here are some from me - including some little metal clay beads :). Im really pleased with the last set - they are wee, really sparkle. The photo dosent show it really :(             










Emma
Emma

Art Clay Senior Instructor & Lampworker

www.emmabaird.wordpress.com

Josephine

Well everyone is very busy this week. Lovely flower beads, and very impressive implosions there Q. I really like those little grey squares with silver dots. Lots of other really nice work too,

Here is a set from me.


julieHB

My friends are really supportive when they look at my efforts of wonky plunged beads and smudged flowerbeads etc., but their eyes only really light up when they see my humble efforts at various critters - so I keep making pigs, cows and penguins (mostly for mobile phone charms), and have recently figured out how to make a sheep....and if anyone has a great tut on how to make a clown I'd really appreciate it  ;D

Julie xx

                           My Webbie - My Flickr

Dragonfire Glass

cute faces on the critters & I love the sheep!

I was asked to make a barn owl


and I made this for a challenge in another forum, but is a bit clown-like

turnedlight

Ooh - all lovely! I made these yesterday, I had planned from the start to etch them, but now I'm not sure..

     
kathryn

glassworks

#192
check out the other thread to see more details....  ;) 8)


Paula

#193
Yesterday, I concentrated on my puckered ends....I do  feel I'm getting there.

I tried colours I wouldnt normally use, and it felt very tropical.



Today, I was trying dots....there were a couple that I was really pleased with, so I hope when cooled  they still look as good.

I am completely addicted!!
Paula

LesleyMac

Gorgeous as ever Mindy, I love your use of colour

Some from me then



A new set




and a silver core with handmade pmc beadcaps, this is big enough to make a nice focal I think.









Lesley
Everyone is gifted, its just that some leave the wrapping on longer than others
(Richard Wilkins)


My Etsy http://www.etsy.com/shop.php?user_id=5469196