mariag

Made some beads for my StepMum (belated Mother's Day gift)
Set of beads for her Troll Bracelet & 2 focals in the same colours ivory & pale blue (loads of reaction in the focals)

The first focal has raked dots & the other has raked stringer lines........just about to go in for a batch anneal so they haven't been cleaned yet!!

Josephine

Here is  a little set from me, my first go with Terranova. I've used a base of silver cinammon.





June

I really like that bead, Dora.

I like those shapes, too, Julie, they've come out well !

Those colours really work well, Lesley, I like that  ;D

I thought I'd post a couple



I quite like the colours in the first bead, but do you think I can remember what they are? !!  The second one was part of my playing around for the focal exchange, but I changed my mind and chose a different one !

Katiequiggle

#138
Ive not done much this week with the kids off school, well I have but not bead stuff, more kids stuff etc  ;D  Anyway I got in the shed yesterday and this morning and made these.

Gorgeous stuff everyone, very colourful.






Kaz

#139
A few from last weekend and the bottom set has just gone into the kiln (fingers crossed!) I love the effect on the first set - it is Sam's Sargasso Sea frit melted into white and it looks just like a tabby cat!




Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

ejralph

Great show and tell everyone

I made a set this week that I almost kept for me!



Emma

sparrow

Wow, Kaz, you must have been working overtime! I love your sets!
Josephine, I love those colours - still have my ASK trial pack, mus have a play with it.
Lesley, next time you doubt *any* of your beads, just send it to me ;)
Dora, I love those florals, I wish I could study with you some time!
Christina, you've inspired me to do more with my pixie dust than dip a whole bead in it - I didn't know that was possible. Love the murrini!
Julie, I like the pods, they'd make a really nice chunky necklace!
June, I love the bottom colours - I'm having a lilac-y time at the mo' - must be spring.
Jaq *sigh*......how very, very pretty  ;D
Oooh, wow Emma, they're lovely - are the bumps frit?


I've been playing with filigrana hollows (I had a red one as well, but lost the bubble, so it kind of doesn't qualify as a 'hollow' any more ;)):

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

emjee

Wow... amazing beads!!!!


I made a new murrini last week!!





Marion

www.emjee-beads.nl
www.emjeebeads.etsy.com

afina

I have something to show today, too.
A latticino bead - I love the Japanese beads that are made this way and would like to manage to do them as beautiful as they do in a few years :)

Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at

Amber


kaatje

Beautiful beads in here, and the week is only 2,5 days old... !

Still have a photo here of a 40mm lentil that I made for Maria Louisa a while ago, in return I got one of her ML-fish:


Love, Karin

Shirley

Val Cox Frit - Thai and Bali Silver 

LesleyMac

Oh this S&T just gets better and better, Marion those murrini are wonderful - you clever girl and the Japanese style bead is gorgeous Verena, I also like the bright colours Amber those are really bright and nice. As for all those beads on that bracelet - amazing - what patience.

I was drooling over my 1000 glass beads book and I just love those Christina Logan beads on the front - so I made a few.





Also made a hollow





and a tube bead from last week





Lesley
Everyone is gifted, its just that some leave the wrapping on longer than others
(Richard Wilkins)


My Etsy http://www.etsy.com/shop.php?user_id=5469196

sparrow

It's still missing a bail, but I thought then I'd stick it on a red velvet ribbon and call it 'Temptation'................

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

afina

Love the dicros!
Here is my latest, a goldtab XL (35mm):
Regards, Verena