Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can't remove them.

A: Soak in water, grip the rod with pliers close to the bead and gently twist the bead.

Try putting them in the freezer for a short while, or soaking in Coke or Cillit Bang - this can help.