There are many different types of torches available to use in glass bead making or lampworking. Many artists start out on the "Hot Head" which uses propane only. Other torches include the Nortel Minor, Carlisle CC, Bethlehem burners and the Lynx to name but a few. These torches make use of dual fuel which means that a source of propane and oxygen is required.