Nortel Minor Burner

The Minor Burner is a surface mix 7 port torch that runs on propane and oxygen or natural gas and oxygen. It is made by Nortel Manufacturing
Developed by Peter Norton in the 1950's it is a well liked torch frequently used for making beads and small scale sculptural work, primarily designed for soft glass
Recommended operating pressures:
- Gas : 0.25 to 5 psi
- Oxygen : 5 to 15 psi
Cleaning and Maintenance
All that is required is for the tubes to be cleaned with the fine needle that is supplied with the torch.