Difference between revisions of "Strain point"
From Fritipedia
Jump to navigationJump to searchLine 6: | Line 6: | ||
==Effetre glass== | ==Effetre glass== | ||
The annealing temp is between 493C - 520C but the strain point is 448C | The annealing temp is between 493C - 520C but the strain point is 448C | ||
+ | |||
+ | ==Bullseye== | ||
+ | The annealing temp is 504C and strain point is 437C |
Revision as of 12:38, 12 November 2008
This is the temperature at which the molecules in the glass stop flowing and moving. Below this point if the bead has not been annealed correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed).
The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the coefficiency of the glass
Effetre glass
The annealing temp is between 493C - 520C but the strain point is 448C
Bullseye
The annealing temp is 504C and strain point is 437C