The Minor Burner is a [[surface mix]] 7 port [[torch]] that runs on [[propane]] and [[oxygen]] or [[natural gas]] and oxygen. It is made by [http://www.nortelmanufacturing.com/torches-minor.shtml Nortel Manufacturing] | The Minor Burner is a [[surface mix]] 7 port [[torch]] that runs on [[propane]] and [[oxygen]] or [[natural gas]] and oxygen. It is made by [http://www.nortelmanufacturing.com/torches-minor.shtml Nortel Manufacturing] | ||
==Information== | |||
Developed by Peter Norton in the 1950's it is a well liked [[torch]] frequently used for making [[beads]] and small scale [[sculptural]] work, primarily designed for [[soft glass]] | Developed by Peter Norton in the 1950's it is a well liked [[torch]] frequently used for making [[beads]] and small scale [[sculptural]] work, primarily designed for [[soft glass]] | ||
Recommended operating pressures: | Recommended operating pressures: | ||
.25 to 5 psi | * Gas : 0.25 to 5 psi | ||
5 to 15 psi | * Oxygen : 5 to 15 psi | ||
====Cleaning and Maintenance==== | ====Cleaning and Maintenance==== | ||
All that is required is for the tubes to be cleaned with the fine needle that is supplied with the torch. | All that is required is for the tubes to be cleaned with the fine needle that is supplied with the torch. | ||
Latest revision as of 22:47, 15 November 2008

The Minor Burner is a surface mix 7 port torch that runs on propane and oxygen or natural gas and oxygen. It is made by Nortel Manufacturing
Information
Developed by Peter Norton in the 1950's it is a well liked torch frequently used for making beads and small scale sculptural work, primarily designed for soft glass
Recommended operating pressures:
- Gas : 0.25 to 5 psi
- Oxygen : 5 to 15 psi
Cleaning and Maintenance
All that is required is for the tubes to be cleaned with the fine needle that is supplied with the torch.