Difference between revisions of "Vetrofond"
From Fritipedia
Jump to navigationJump to searchm (made headings) |
(reformatted tabl to split stock numbers) |
||
Line 6: | Line 6: | ||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
+ | ! Stock Number | ||
! Colour | ! Colour | ||
! Properties | ! Properties | ||
! Reactions | ! Reactions | ||
|- | |- | ||
− | | 1004 clear | + | | 1004 |
+ | | clear | ||
| Colours appear lighter encased in clear | | Colours appear lighter encased in clear | ||
| | | | ||
|- | |- | ||
− | | 1005 crystal clear | + | | 1005 |
+ | | crystal clear | ||
| good for encasing silver glass | | good for encasing silver glass | ||
| | | | ||
|- | |- | ||
− | | 1008 yellow | + | | 1008 |
+ | | yellow | ||
| | | | ||
| | | | ||
|- | |- | ||
− | | 1012 light topaz | + | | 1012 |
+ | | light topaz | ||
| | | | ||
| | | | ||
|- | |- | ||
− | | 1014 topaz | + | | 1014 |
+ | | topaz | ||
| | | | ||
| Reacts with DH psyche to give purples and blues | | Reacts with DH psyche to give purples and blues | ||
|- | |- | ||
− | | 1020 light grass green | + | | 1020 |
+ | | light grass green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | | 1022 grass green | + | | 1022 |
+ | | grass green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | | 1024 dark grass green | + | | 1024 |
+ | | dark grass green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | | 1026 teal | + | | 1026 |
+ | | teal | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1028 light emerald green | + | | 1028 |
+ | | light emerald green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1030 emerald green | + | | 1030 |
+ | | emerald green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1034 light aquamarine | + | | 1034 |
+ | | light aquamarine | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1036 aquamarine (aqua) | + | | 1036 |
+ | | aquamarine (aqua) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1038 pale aquamarine (light aqua) | + | | 1038 |
+ | | pale aquamarine (light aqua) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1040 light purple | + | | 1040 |
+ | | light purple | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1042 purple | + | | 1042 |
+ | | purple | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1044 dark purple | + | | 1044 |
+ | | dark purple | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1048 grey | + | | 1048 |
+ | | grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1052 light blue | + | | 1052 |
+ | | light blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1054 blue | + | | 1054 |
+ | | blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1058 intense blue | + | | 1058 |
+ | | intense blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1060 cobalt blue | + | | 1060 |
+ | | cobalt blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1064 black | + | | 1064 |
+ | | black | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1068 pink | + | | 1068 |
+ | | pink | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1069 electric yellow | + | | 1069 |
+ | | electric yellow | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1072 orange | + | | 1072 |
+ | | orange | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1076 red | + | | 1076 |
+ | | red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1080 pale lavender | + | | 1080 |
+ | | pale lavender | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1082 lavender blue (alexandrite) | + | | 1082 |
+ | | lavender blue (alexandrite) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1084 light brown | + | | 1084 |
+ | | light brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1086 medium brown | + | | 1086 |
+ | | medium brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1088 dark brown | + | | 1088 |
+ | | dark brown | ||
| | | | ||
| | | | ||
Line 143: | Line 176: | ||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
+ | ! Stock Number | ||
! Colour | ! Colour | ||
! Properties | ! Properties | ||
! Reactions | ! Reactions | ||
|- | |- | ||
− | |1204 white | + | |1204 |
+ | |white | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1206 anice white | + | |1206 |
+ | |anice white | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1208 silk white | + | |1208 |
+ | |silk white | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1212 pea green | + | |1212 |
+ | |pea green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1214 nile green | + | |1214 |
+ | |nile green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1216 grass green | + | |1216 |
+ | |grass green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1218 dark grass green | + | |1218 |
+ | |dark grass green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1220 periwinkle | + | |1220 |
+ | |periwinkle | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1224 light sky blue | + | |1224 |
+ | |light sky blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1228 dark sky blue | + | |1228 |
+ | |dark sky blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1232 turquoise | + | |1232 |
+ | |turquoise | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1236 dark turquoise | + | |1236 |
+ | |dark turquoise | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1240 light lapis blue | + | |1240 |
+ | |light lapis blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1242 lapis blue | + | |1242 |
+ | |lapis blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1246 cobalt blue | + | |1246 |
+ | |cobalt blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1248 light grey | + | |1248 |
+ | |light grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1250 medium grey | + | |1250 |
+ | |medium grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1255 flower pink | + | |1255 |
+ | |flower pink | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1262 dark ivory | + | |1262 |
+ | |dark ivory | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1264 light ivory | + | |1264 |
+ | |light ivory | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1268 pearl grey | + | |1268 |
+ | |pearl grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1272 violet | + | |1272 |
+ | |violet | ||
| | | | ||
| | | | ||
Line 242: | Line 298: | ||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
+ | ! Stock Number | ||
! Colour | ! Colour | ||
! Properties | ! Properties | ||
! Reactions | ! Reactions | ||
|- | |- | ||
− | |1408 medium yellow | + | |1408 |
+ | |medium yellow | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1412 dark lemon | + | |1412 |
+ | |dark lemon | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1420 coral | + | |1420 |
+ | |coral | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1424 carrot red | + | |1424 |
+ | |carrot red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1428 light red | + | |1428 |
+ | |light red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1432 medium red | + | |1432 |
+ | |medium red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1438 red purple | + | |1438 |
+ | |red purple | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1444 light brown | + | |1444 |
+ | |light brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |448 dark brown | + | |448 |
+ | |dark brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1456 gold pink | + | |1456 |
+ | |gold pink | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1460 yellow ocher (wasabi) | + | |1460 |
+ | |yellow ocher (wasabi) | ||
| | | | ||
| | | | ||
Line 295: | Line 363: | ||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
+ | ! Stock Number | ||
! Colour | ! Colour | ||
! Properties | ! Properties | ||
! Reactions | ! Reactions | ||
|- | |- | ||
− | |1801 cosmic storm | + | |1801 |
+ | |cosmic storm | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1802 apricot jam | + | |1802 |
+ | |apricot jam | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1803 candy corn | + | |1803 |
+ | |candy corn | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1804 tomato soup | + | |1804 |
+ | |tomato soup | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1805 orange dreamsicle | + | |1805 |
+ | |orange dreamsicle | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1806 smoke rings | + | |1806 |
+ | |smoke rings | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1807 frog pond | + | |1807 |
+ | |frog pond | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1808 swamp moss | + | |1808 |
+ | |swamp moss | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1809 jungle twilight | + | |1809 |
+ | |jungle twilight | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1810 lemongrass | + | |1810 |
+ | |lemongrass | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1811 moon rock | + | |1811 |
+ | |moon rock | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1906 chardonnay | + | |1906 |
+ | |chardonnay | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1909 transparent green odd | + | |1909 |
+ | |transparent green odd | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1910 transparent yellow odd | + | |1910 |
+ | |transparent yellow odd | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1911 silk white (opal white) | + | |1911 |
+ | |silk white (opal white) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1912 olive green pastel | + | |1912 |
+ | |olive green pastel | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1917 Transparent amber (streaky amber)(antique amber) | + | |1917 |
+ | |Transparent amber (streaky amber)(antique amber) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1919 pale ivory | + | |1919 |
+ | |pale ivory | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1922 transparent sage green | + | |1922 |
+ | |transparent sage green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1925 transparent pale blue | + | |1925 |
+ | |transparent pale blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1926 sea green (seafoam) | + | |1926 |
+ | |sea green (seafoam) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1927 ocean green | + | |1927 |
+ | |ocean green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1931 river rock (brie)(avocado) | + | |1931 |
+ | |river rock (brie)(avocado) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1932 fish pink | + | |1932 |
+ | |fish pink | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1933 pink no.3 | + | |1933 |
+ | |pink no.3 | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1934 pink flower | + | |1934 |
+ | |pink flower | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1937 arancio perfecto | + | |1937 |
+ | |arancio perfecto | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1938 pale aqua streaky | + | |1938 |
+ | |pale aqua streaky | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1939 intense tangerine | + | |1939 |
+ | |intense tangerine | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1943 orange sherbert (free range salmon pink) | + | |1943 |
+ | |orange sherbert (free range salmon pink) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1940 italian marble | + | |1940 |
+ | |italian marble | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1941 pineapple yellow | + | |1941 |
+ | |pineapple yellow | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1942 watermelon (poppy) | + | |1942 |
+ | |watermelon (poppy) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1944 tangerine | + | |1944 |
+ | |tangerine | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1945 new white (custard) | + | |1945 |
+ | |new white (custard) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1946 sunshine 1947 yellow ice (lemon ice)(belgian lace) | + | |1946 |
+ | |sunshine 1947 yellow ice (lemon ice)(belgian lace) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1948 banana cream | + | |1948 |
+ | |banana cream | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1949 lemon meringue | + | |1949 |
+ | |lemon meringue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1951 transparent candy apple red | + | |1951 |
+ | |transparent candy apple red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1952 violet odd (purplicious) | + | |1952 |
+ | |violet odd (purplicious) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1954 cool white (odd cotton) | + | |1954 |
+ | |cool white (odd cotton) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1955 seashell swirl | + | |1955 |
+ | |seashell swirl | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1957 orange punch | + | |1957 |
+ | |orange punch | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1958 pyjama blue | + | |1958 |
+ | |pyjama blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1960 light pink | + | |1960 |
+ | |light pink | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1961 carrot red | + | |1961 |
+ | |carrot red | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1963 green tepenade | + | |1963 |
+ | |green tepenade | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1964 pale avocado | + | |1964 |
+ | |pale avocado | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1965 olive green | + | |1965 |
+ | |olive green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1966 dark olive green | + | |1966 |
+ | |dark olive green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1967 quartz grey | + | |1967 |
+ | |quartz grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1968 slate blue | + | |1968 |
+ | |slate blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1969 pearl grey | + | |1969 |
+ | |pearl grey | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1970 transparent streaky sapphire | + | |1970 |
+ | |transparent streaky sapphire | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1975 midnight blue | + | |1975 |
+ | |midnight blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1976 key lime green | + | |1976 |
+ | |key lime green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1977 parrot green | + | |1977 |
+ | |parrot green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1978 transparent crystal green | + | |1978 |
+ | |transparent crystal green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1980 light streaky brown | + | |1980 |
+ | |light streaky brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1981 streaky brown | + | |1981 |
+ | |streaky brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1982 dark streaky brown | + | |1982 |
+ | |dark streaky brown | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1983 pale ocean blue | + | |1983 |
+ | |pale ocean blue | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1984 pale moss agate | + | |1984 |
+ | |pale moss agate | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1985 moss agate | + | |1985 |
+ | |moss agate | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1986 lichen | + | |1986 |
+ | |lichen | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1987 dark lichen | + | |1987 |
+ | |dark lichen | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1988 pale crystal green | + | |1988 |
+ | |pale crystal green | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1989 transparent odd topaz | + | |1989 |
+ | |transparent odd topaz | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1990 honey crunch | + | |1990 |
+ | |honey crunch | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1991 marbled avocado | + | |1991 |
+ | |marbled avocado | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1992 banana | + | |1992 |
+ | |banana | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1993 sweet lime (red jasper) | + | |1993 |
+ | |sweet lime (red jasper) | ||
| | | | ||
| | | | ||
|- | |- | ||
− | |1994 strawberry sweet (dark red jasper) | + | |1994 |
+ | |strawberry sweet (dark red jasper) | ||
| | | | ||
| | | | ||
|- | |- | ||
|} | |} |
Revision as of 15:51, 14 November 2008
Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number. Vetrofond colours and stock numbers
Transparent
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1004 | clear | Colours appear lighter encased in clear | |
1005 | crystal clear | good for encasing silver glass | |
1008 | yellow | ||
1012 | light topaz | ||
1014 | topaz | Reacts with DH psyche to give purples and blues | |
1020 | light grass green | ||
1022 | grass green | ||
1024 | dark grass green | ||
1026 | teal | ||
1028 | light emerald green | ||
1030 | emerald green | ||
1034 | light aquamarine | ||
1036 | aquamarine (aqua) | ||
1038 | pale aquamarine (light aqua) | ||
1040 | light purple | ||
1042 | purple | ||
1044 | dark purple | ||
1048 | grey | ||
1052 | light blue | ||
1054 | blue | ||
1058 | intense blue | ||
1060 | cobalt blue | ||
1064 | black | ||
1068 | pink | ||
1069 | electric yellow | ||
1072 | orange | ||
1076 | red | ||
1080 | pale lavender | ||
1082 | lavender blue (alexandrite) | ||
1084 | light brown | ||
1086 | medium brown | ||
1088 | dark brown |
Opaque/pastels
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1204 | white | ||
1206 | anice white | ||
1208 | silk white | ||
1212 | pea green | ||
1214 | nile green | ||
1216 | grass green | ||
1218 | dark grass green | ||
1220 | periwinkle | ||
1224 | light sky blue | ||
1228 | dark sky blue | ||
1232 | turquoise | ||
1236 | dark turquoise | ||
1240 | light lapis blue | ||
1242 | lapis blue | ||
1246 | cobalt blue | ||
1248 | light grey | ||
1250 | medium grey | ||
1255 | flower pink | ||
1262 | dark ivory | ||
1264 | light ivory | ||
1268 | pearl grey | ||
1272 | violet |
Specials
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1408 | medium yellow | ||
1412 | dark lemon | ||
1420 | coral | ||
1424 | carrot red | ||
1428 | light red | ||
1432 | medium red | ||
1438 | red purple | ||
1444 | light brown | ||
448 | dark brown | ||
1456 | gold pink | ||
1460 | yellow ocher (wasabi) |
Odd lots
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1801 | cosmic storm | ||
1802 | apricot jam | ||
1803 | candy corn | ||
1804 | tomato soup | ||
1805 | orange dreamsicle | ||
1806 | smoke rings | ||
1807 | frog pond | ||
1808 | swamp moss | ||
1809 | jungle twilight | ||
1810 | lemongrass | ||
1811 | moon rock | ||
1906 | chardonnay | ||
1909 | transparent green odd | ||
1910 | transparent yellow odd | ||
1911 | silk white (opal white) | ||
1912 | olive green pastel | ||
1917 | Transparent amber (streaky amber)(antique amber) | ||
1919 | pale ivory | ||
1922 | transparent sage green | ||
1925 | transparent pale blue | ||
1926 | sea green (seafoam) | ||
1927 | ocean green | ||
1931 | river rock (brie)(avocado) | ||
1932 | fish pink | ||
1933 | pink no.3 | ||
1934 | pink flower | ||
1937 | arancio perfecto | ||
1938 | pale aqua streaky | ||
1939 | intense tangerine | ||
1943 | orange sherbert (free range salmon pink) | ||
1940 | italian marble | ||
1941 | pineapple yellow | ||
1942 | watermelon (poppy) | ||
1944 | tangerine | ||
1945 | new white (custard) | ||
1946 | sunshine 1947 yellow ice (lemon ice)(belgian lace) | ||
1948 | banana cream | ||
1949 | lemon meringue | ||
1951 | transparent candy apple red | ||
1952 | violet odd (purplicious) | ||
1954 | cool white (odd cotton) | ||
1955 | seashell swirl | ||
1957 | orange punch | ||
1958 | pyjama blue | ||
1960 | light pink | ||
1961 | carrot red | ||
1963 | green tepenade | ||
1964 | pale avocado | ||
1965 | olive green | ||
1966 | dark olive green | ||
1967 | quartz grey | ||
1968 | slate blue | ||
1969 | pearl grey | ||
1970 | transparent streaky sapphire | ||
1975 | midnight blue | ||
1976 | key lime green | ||
1977 | parrot green | ||
1978 | transparent crystal green | ||
1980 | light streaky brown | ||
1981 | streaky brown | ||
1982 | dark streaky brown | ||
1983 | pale ocean blue | ||
1984 | pale moss agate | ||
1985 | moss agate | ||
1986 | lichen | ||
1987 | dark lichen | ||
1988 | pale crystal green | ||
1989 | transparent odd topaz | ||
1990 | honey crunch | ||
1991 | marbled avocado | ||
1992 | banana | ||
1993 | sweet lime (red jasper) | ||
1994 | strawberry sweet (dark red jasper) |