− | This is the | + | This is the temperature at which the molecules in the glass stop flowing and moving. |
+ | Below this point if the bead has not been [[annealing|annealed]] correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed). | ||
+ | |||
+ | The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the [[coefficiency]] of the glass |
Revision as of 09:35, 12 November 2008
This is the temperature at which the molecules in the glass stop flowing and moving. Below this point if the bead has not been annealed correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed).
The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the coefficiency of the glass