User contributions
From Fritipedia
Jump to navigationJump to search- 07:08, 24 September 2010 diff hist +298 N Removing beads from mandrel New page: Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can't remove them. A: Soak in water, grip the rod with pliers close to the bead and gently twist th... current
- 07:04, 24 September 2010 diff hist +1 Lampworking →Beginners Lampworking Q&A current
- 07:03, 24 September 2010 diff hist +32 Lampworking →Beginners Lampworking Q&A
- 07:04, 23 September 2010 diff hist +266 N Amber/purple New page: The term 'amber/purple' generally refers to glass that absorbs amber light and reflects purples - in a dull room, the glass will appear amber coloured, but with good light, or in bright su... current
- 06:59, 23 September 2010 diff hist +671 N Coefficient of Expansion New page: COE, or Coefficient of Expansion, describes by how much a material will expand per degree of temperature increase. Different types of glass have different COE's. Glass, like many material...
- 06:52, 23 September 2010 diff hist +425 N Borosilicate Glass New page: Borosilicate glass, often just referred to as 'boro' or 'hard glass', has a COE of 33. This glass needs a higher temperature to melt and is generallly stiffer when molten than glass wi... current
- 06:26, 23 September 2010 diff hist +1 Glass Alchemy current
- 06:25, 23 September 2010 diff hist +1 Northstar 33 current
- 06:25, 23 September 2010 diff hist +65 N Borostix New page: Borostix are a range of opaque non-reactive borosilicate colours. current
- 06:24, 23 September 2010 diff hist +312 N Momka New page: Momka's glass makes a range of borosilicate glass coloured rods. Frit is also available from the distributor listed on the [http://www.momkasglass.com/ manufacturer's website]. Working ti... current
- 06:22, 23 September 2010 diff hist +268 N Glass Alchemy New page: Glass Alchemy manufacture a wide range of boroslicate glass colour rods as well as frit in a variety of grades and coloured tubing. Working tips and information on the range of colours of...
- 06:20, 23 September 2010 diff hist +242 N Northstar 33 New page: Northstar manufacture a wide range of boroslicate glass colours as well as frit in a variety of grades. Working tips and information on the range of colours offered can be found on the [h...
- 06:15, 23 September 2010 diff hist +130 TAG 33 current
- 06:11, 23 September 2010 diff hist +107 N TAG 33 New page: TAG 33 is made by [Trautman Art Glass] who manufacture a range of colours as well as a small range of frit.
- 06:08, 23 September 2010 diff hist +218 Glass →Which glass should I use to make beads from?
- 05:54, 23 September 2010 diff hist -1 Lampworking
- 05:54, 23 September 2010 diff hist -8 Lampworking →How is it done
- 05:53, 23 September 2010 diff hist +8 Lampworking →How is it done
- 04:18, 23 September 2010 diff hist +419 N Poking hot glass New page: Q - "I have a tungsten pick and also a rake, but both tools get stuck in the glass" A - If your tools are hot they will stick to the glass. Try to keep your tools out of the flame. If you... current
- 04:13, 23 September 2010 diff hist +56 Lampworking →How is it done
- 08:55, 2 December 2008 diff hist +4 Reichenbach
- 08:54, 2 December 2008 diff hist +132 Reichenbach
- 05:27, 16 November 2008 diff hist +4 Double Helix
- 05:25, 16 November 2008 diff hist +101 N Precision 104 New page: A range of silver-rich C0E104 rods for beadmaking produced by Northstar glassworks in the US. current
- 05:22, 16 November 2008 diff hist +231 N Kugler New page: Kugler are a German Company producing three separate ranges of glass for glassworking. Kugler Colors rods are CoE 93 while the Beadmaking 104 range is CoE 104. Kugler manufactured the no-l...
- 05:17, 16 November 2008 diff hist +20 Glass →Which glass should I use to make beads from?
- 05:15, 16 November 2008 diff hist +99 N Double Helix New page: Double Helix, based in the US, produce a range of silver rich glass rods and frit that are CoE 104.
- 06:45, 12 November 2008 diff hist +47 Sandpit →YES!!! I too have edited the wiki and am a wiki virgin no longer!!
- 06:44, 12 November 2008 diff hist -120 Sandpit →Wiki Editing Game!!! Log in (FHF username & p'word), click 'Edit' and add your name to the bottom of the list!
- 06:44, 12 November 2008 diff hist +13 Sandpit →Wiki Editing Game!!! Log in (FHF username & p'word), click 'Edit' and add your name to the bottom of the list!
- 06:44, 12 November 2008 diff hist +106 Sandpit →Wiki Editing Game!!! Log in (FHF username & p'word), click 'Edit' and add your name to the bottom of the list!