  • curprev 07:08, 24 September 2010Garishglobes talk contribs 298 bytes +298 New page: Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can't remove them. A: Soak in water, grip the rod with pliers close to the bead and gently twist th...