Reichenbach produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenbach 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down. Reichenbach also produce a range of CoE92 glass rods and frits, many of which are either reactive or reducing colours.
Reichenbach colours and stock numbers
Transparent
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
L1011 | Crystal | clear | |
L1012 | Crystal soft | soft clear | |
L2011 | Violet reddish | ||
L2012 | Gold violet | more violet than rubino | |
L2013 | Gold ruby light | ||
L2015 | Pink lady | ||
L4015 | Antique | aka antique clear, is greenish | |
L5010 | Silver brown | silver reduction glass | |
L6015 | Garnet red | ||
L6027 | Rosalin | ||
L7003 | Amber | ||
L9202 | Black | ||
L5011 | Dark silver brown | silver reduction glass | |
L9203 | Deep black | may reduce metallic | |
L1012B | Ocean | blue with sparkles | |
L1012G | Antique green | aka antique sparkle (is not green!) |
Opaque
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
L1200 | White | ||
L2201 | Soft violet | ||
L2207 | Iris violet | Reduces to metallic | |
L3018 | Middle blue | ||
L3206 | Iris dense blue | Reduces to metallic | |
L4010 | Iris green | Reduces to metallic | |
L4016 | Beryl green | ||
L4205 | Middle green | ||
L4207 | Light green | ||
L5210 | Opal yellow | ||
L6116 | Lipstick | ||
L6208 | Iris orange | aka raku | strikes to multicolour (also reduces to metallic) |
L6210 | Magic | strikes to multicolour | |
L6212 | Dark red | ||
L6213 | Strawberry | ||
L6214 | Opal orange | ||
L6215 | Light red | ||
L6219 | Opal raspberry | ||
L7205 | Caramel | reduces to metallic | |
L7206 | Scarlet brown | ||
L6209 | Multicolour | strikes multicolour green-blue | |
L6218 | Flamingo | reduces to metallic | |
L7202 | Porcelain | ||
L6221 | Lilac | ||
L6202 | Multicolour dark | strikes multicolour green-blue-purple-red |
Mystics and Pearls
These have a shampoo-like sheen, can be semi-translucent and variegated colour.
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
L201 | Mystic violet | ||
L301 | Mystic blue | ||
L401 | Mystic green | ||
L501 | Mystic yellow | ||
L502 | Mystic orange | ||
L601 | Mystic pink | ||
L605 | Mystic red | ||
L701 | Mystic beige | ||
L801 | Mystic grey | ||
L803 | Mystic grey blue | ||
L201S | Pearl violet | ||
L601S | Pearl pink | ||
L701S | Pearl beige |