− | + | Reichenbach produce a limited range of colours in [[CoE]] 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the [[opaque]] Reichenbach 104 [[glass]]es on a base bead of a very soft [[opaque]] colour (for example [[Effetre]] White) have a "bleed" effect rather than a crisp edge when melted down. | |
<!-- Please leave this at the bottom --> | <!-- Please leave this at the bottom --> | ||
[[Category:Types of Glass]] | [[Category:Types of Glass]] |
Revision as of 19:36, 14 November 2008
Reichenbach produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenbach 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down.