  • curprev 04:18, 23 September 2010Garishglobes talk contribs 419 bytes +419 New page: Q - "I have a tungsten pick and also a rake, but both tools get stuck in the glass" A - If your tools are hot they will stick to the glass. Try to keep your tools out of the flame. If you...