(New page: ==Nortel Minor Burner== The Minor Burner is a surface mix 7 port torch that runs on propane and oxygen or natural gas and oxygen. It is made by Nortel Manufacturing [http://www.nortelman...)
 
m (modified links)
Line 1: Line 1:
 
==Nortel Minor Burner==
 
==Nortel Minor Burner==
  
The Minor Burner is a surface mix 7 port torch that runs on propane and oxygen or natural gas and oxygen. It is made by Nortel Manufacturing [http://www.nortelmanufacturing.com/torches-minor.shtml]
+
The Minor Burner is a [[surface mix]] 7 port torch that runs on [[propane]] and [[oxygen]] or [[natural gas]] and oxygen. It is made by [http://www.nortelmanufacturing.com/torches-minor.shtml Nortel Manufacturing]
  
Developed by Peter Norton in the 1950's it is a well liked torch frequently used for making beads and small scale sculptural work, primarily designed for soft glass
+
Developed by Peter Norton in the 1950's it is a well liked [[torch]] frequently used for making [[beads]] and small scale [[sculptural]] work, primarily designed for [[soft glass]]
  
 
Recommended operating pressures:
 
Recommended operating pressures:

Revision as of 08:41, 13 November 2008

Nortel Minor Burner

The Minor Burner is a surface mix 7 port torch that runs on propane and oxygen or natural gas and oxygen. It is made by Nortel Manufacturing

Developed by Peter Norton in the 1950's it is a well liked torch frequently used for making beads and small scale sculptural work, primarily designed for soft glass

Recommended operating pressures: .25 to 5 psi gas 5 to 15 psi oxygen

Cleaning and Maintenance

All that is required is for the tubes to be cleaned with the fine needle that is supplied with the torch.