Kugler
From Fritipedia
Revision as of 05:22, 16 November 2008 by Garishglobes (talk | contribs) (New page: Kugler are a German Company producing three separate ranges of glass for glassworking. Kugler Colors rods are CoE 93 while the Beadmaking 104 range is CoE 104. Kugler manufactured the no-l...)
Kugler are a German Company producing three separate ranges of glass for glassworking. Kugler Colors rods are CoE 93 while the Beadmaking 104 range is CoE 104. Kugler manufactured the no-longer produced ASK 104 rods for beadmaking.