Difference between revisions of "Evil Devitrifying Purple"
From Fritipedia
Jump to navigationJump to search (New page: ==EDP - Evil Devitrifying Purple== An Effetre handpulled colour, number 254. Opaque glass that produces a range of lovely purples. Named EDP because of its tendency to devitrify - loo...) |
|||
Line 1: | Line 1: | ||
− | + | Otherwise known as Evil Devitrifying Purple | |
− | An Effetre handpulled colour, number 254. Opaque glass that produces a range of lovely purples. Named EDP because of its tendency to [[devitrify]] - loose its glassy ness - when worked in certain temperature zones, you will see the glass go rough looking, it is possible to get rid of the devitrification by heating the glass. | + | An [[Effetre]] [[handpulled]] colour, number 254. [[Opaque]] [[glass]] that produces a range of lovely purples. Named EDP because of its tendency to [[devitrify]] - loose its glassy-ness - when worked in certain temperature zones, you will see the glass go rough looking, it is possible to get rid of the [[devitrification]] by heating the [[glass]]. |
− | + | There is a good tutorial on wet canvas about how to work EDP [http://www.wetcanvas.com/forums/showthread.php?t=120817&highlight=sweet+dreamy+purple here]. |
Revision as of 16:58, 19 November 2008
Otherwise known as Evil Devitrifying Purple
An Effetre handpulled colour, number 254. Opaque glass that produces a range of lovely purples. Named EDP because of its tendency to devitrify - loose its glassy-ness - when worked in certain temperature zones, you will see the glass go rough looking, it is possible to get rid of the devitrification by heating the glass.
There is a good tutorial on wet canvas about how to work EDP here.