Difference between revisions of "CiM"

From Fritipedia
Jump to navigationJump to search
Line 21: Line 21:
 
|bordello
 
|bordello
 
|
 
|
|
+
|semi translucent deep red
 
|  
 
|  
 
|-
 
|-
Line 27: Line 27:
 
|Sangre
 
|Sangre
 
|
 
|
|
+
|opaque red
 
|  
 
|  
 
|-
 
|-
Line 33: Line 33:
 
|lipstick
 
|lipstick
 
|
 
|
|  
+
|opaque red brown
 
|  
 
|  
 
|-
 
|-
Line 39: Line 39:
 
|pumpkin
 
|pumpkin
 
|
 
|
|  
+
|opaque light orange
 
|  
 
|  
 
|-
 
|-
Line 45: Line 45:
 
|clockwork
 
|clockwork
 
|
 
|
|  
+
|opaque deep orange
 
|
 
|
 
|-
 
|-
Line 51: Line 51:
 
|creamsicle
 
|creamsicle
 
|
 
|
|  
+
|semi opaque orange
 
|
 
|
 
|-
 
|-
Line 57: Line 57:
 
|ghee
 
|ghee
 
|
 
|
|  
+
|semi opaque light yellow
 
|  
 
|  
 
|-
 
|-
Line 63: Line 63:
 
|stoneground
 
|stoneground
 
|
 
|
|
+
|opaque light brown
 
|
 
|
 
|-
 
|-
Line 69: Line 69:
 
|cedalon
 
|cedalon
 
|
 
|
|
+
|opaque turquoise
 
|  
 
|  
 
|-
 
|-
Line 75: Line 75:
 
|peacock green
 
|peacock green
 
|
 
|
|
+
|semi transparent light green
 
|
 
|
 
|-
 
|-
Line 81: Line 81:
 
|elphaba
 
|elphaba
 
|
 
|
|
+
|opaque light green
 
|
 
|
 
|-
 
|-
Line 87: Line 87:
 
|dirty martini
 
|dirty martini
 
|
 
|
|
+
|opaque pale green
 
|
 
|
 
|-
 
|-
Line 93: Line 93:
 
|kryptonite
 
|kryptonite
 
|
 
|
|
+
|semi opaque light blue
 
|
 
|
 
|-
 
|-
Line 99: Line 99:
 
|french blue
 
|french blue
 
|
 
|
|
+
|opaque bright blue
 
|
 
|
 
|-
 
|-
Line 105: Line 105:
 
|leaky pen
 
|leaky pen
 
|
 
|
|
+
|semi translucent dark blue
 
|
 
|
 
|-
 
|-
Line 111: Line 111:
 
|halong bay
 
|halong bay
 
|
 
|
|
+
|semi translucent light blue
 
|
 
|
 
|-
 
|-
Line 117: Line 117:
 
|glacier
 
|glacier
 
|
 
|
|
+
|opaque light blue
 
|
 
|
 
|-
 
|-
Line 123: Line 123:
 
|lapis
 
|lapis
 
|
 
|
|
+
|opaque purple blue
 
|
 
|
 
|-
 
|-
 
|C0543
 
|C0543
|sapphire blue
+
|sapphire
|
 
 
|
 
|
 +
|transparent medium blue
 
|
 
|
 
|-
 
|-
Line 135: Line 135:
 
|electric avenue
 
|electric avenue
 
|
 
|
|
+
|opaque medium blue
 
|
 
|
 
|-
 
|-
Line 141: Line 141:
 
|chalcedony
 
|chalcedony
 
|
 
|
|
+
|opaque light blue
 
|
 
|
 
|-
 
|-
Line 147: Line 147:
 
|ming
 
|ming
 
|
 
|
|
+
|opaque deep blue
 
|
 
|
 
|-
 
|-
 
|C0563
 
|C0563
|ming
+
|pulsar
|
 
 
|
 
|
 +
|transparent medium blue
 
|
 
|
 
|-
 
|-
Line 159: Line 159:
 
|simply berry
 
|simply berry
 
|
 
|
|
+
|semi opaque light purple
 
|
 
|
 
|-
 
|-
Line 165: Line 165:
 
|thai orchid
 
|thai orchid
 
|
 
|
|
+
|opaque violet
 
|
 
|
 
|-
 
|-
Line 171: Line 171:
 
|heffalump
 
|heffalump
 
|
 
|
|
+
|opaque pale lilac
 
|
 
|
 
|-
 
|-
Line 177: Line 177:
 
|count von count
 
|count von count
 
|
 
|
|
+
|transparent light purple
 
|
 
|
 
|-
 
|-
Line 183: Line 183:
 
|larkspur
 
|larkspur
 
|
 
|
|
+
|transparent pale purple
 
|
 
|
 
|-
 
|-
Line 189: Line 189:
 
|grape ape
 
|grape ape
 
|
 
|
|
+
|opaque medium purple
 
|
 
|
 
|-
 
|-
Line 195: Line 195:
 
|eggplant
 
|eggplant
 
|
 
|
|
+
|opaque dark purple
 
|
 
|
 
|-
 
|-
Line 201: Line 201:
 
|plum
 
|plum
 
|
 
|
|
+
|semi translucent light purple
 
|
 
|
 
|-
 
|-
Line 207: Line 207:
 
|crocus
 
|crocus
 
|
 
|
|
+
|semi opaque light purple
 
|
 
|
 
|-
 
|-
Line 213: Line 213:
 
|evil queen
 
|evil queen
 
|
 
|
|
+
|opaque deep purple
 
|
 
|
 
|-
 
|-
Line 219: Line 219:
 
|poi
 
|poi
 
|
 
|
 +
|opaque dark lilac
 +
|
 +
|-
 +
|C0701
 +
|ginger
 
|
 
|
 +
|opaque light pink
 
|
 
|
 
|-
 
|-
|C0701
+
|C0703
 +
|butter pecan
 +
|
 +
|opaque pale pink
 +
|
 +
|-
 +
|C0717
 
|khaki
 
|khaki
 
|
 
|
|
+
|opaque gray green
 
|
 
|
 
|-
 
|-
Line 231: Line 243:
 
|canyon de chelly
 
|canyon de chelly
 
|
 
|
|
+
|opaque light brown
 
|
 
|
 
|-
 
|-
Line 237: Line 249:
 
|sepia
 
|sepia
 
|
 
|
|
+
|transparent pale pink
 
|
 
|
 
|-
 
|-
Line 243: Line 255:
 
|chai
 
|chai
 
|
 
|
|
+
|opaque pale pink
 
|
 
|
 
|-
 
|-
Line 249: Line 261:
 
|cirrus
 
|cirrus
 
|
 
|
|
+
|semi opaque white
 
|
 
|
 
|-
 
|-
Line 255: Line 267:
 
|hades
 
|hades
 
|
 
|
|
+
|opaque intense black
 
|
 
|
 
|-
 
|-
Line 261: Line 273:
 
|clear
 
|clear
 
|
 
|
|
+
|transparent clear
 
|
 
|
 
|-
 
|-
Line 267: Line 279:
 
|peace
 
|peace
 
|
 
|
|
+
|shimmering opaque white
 
|
 
|
 
|-
 
|-
Line 273: Line 285:
 
|marshmallow
 
|marshmallow
 
|
 
|
|
+
|semi opaque white
 
|
 
|
 
|-
 
|-
Line 279: Line 291:
 
|gelly's sty
 
|gelly's sty
 
|
 
|
|
+
|opaque  light pink
 
|
 
|
 
|-
 
|-
Line 285: Line 297:
 
|rose quartz
 
|rose quartz
 
|
 
|
|
+
|semi opaque light pink
 
|
 
|
 
|-
 
|-
Line 291: Line 303:
 
|pink champagne
 
|pink champagne
 
|
 
|
|
+
|translucent light pink
 
|
 
|
 
|-
 
|-
Line 297: Line 309:
 
|blush
 
|blush
 
|
 
|
|
+
|translucent pale pink
 
|
 
|
 
|-
 
|-
Line 303: Line 315:
 
|cranberry
 
|cranberry
 
|
 
|
|
+
|semi opaque rich dark pink
 
|
 
|
 
|-
 
|-
Line 309: Line 321:
 
|desert pink
 
|desert pink
 
|
 
|
|
+
|opaque pale pink
 
|
 
|
 
|-
 
|-
 
|}
 
|}
 +
 +
 +
=== CiM Uniques ===
  
  

Revision as of 18:58, 8 January 2009

CIM stands for Creation Is Messy. They are suppliers of glass which hs a CoE of 104 and is compatible with Effetre, Vetrofond, Lauscha and the other 104 glasses. The messy colour pallettes are being extended regularly with new shades. They also produce a range of CoE 96 glass called Messy 96. Messy colour 104 and Messy 96 are not compatible.

Occasionally CiM produce a pull of glass that does conform exactly to their colour specifications or one that is created for a test run. These occasional odd lots of glass are labled as "Messy Uniques" and are sold exclusively by Frantz art glass and associated sellers in the U.S.A.

Creation in Messy 104 colours and stock numbers

Information on the working properties of CiM glass is a current research project by members of the Frit-Happens community in the form of a prize competition Frit-Happens CiM Competition Thread

CiM 104

Stock Number Colour Properties Other Info Reactions
C0109 bordello semi translucent deep red
C0128 Sangre opaque red
C0149 lipstick opaque red brown
C0223 pumpkin opaque light orange
C0229 clockwork opaque deep orange
C0241 creamsicle semi opaque orange
C0346 ghee semi opaque light yellow
C0351 stoneground opaque light brown
C0402 cedalon opaque turquoise
C0413 peacock green semi transparent light green
C0430 elphaba opaque light green
C0448 dirty martini opaque pale green
C0449 kryptonite semi opaque light blue
C0505 french blue opaque bright blue
C0508 leaky pen semi translucent dark blue
C0512 halong bay semi translucent light blue
C0519 glacier opaque light blue
C0531 lapis opaque purple blue
C0543 sapphire transparent medium blue
C0547 electric avenue opaque medium blue
C0550 chalcedony opaque light blue
C0562 ming opaque deep blue
C0563 pulsar transparent medium blue
C0618 simply berry semi opaque light purple
C0632 thai orchid opaque violet
C0645 heffalump opaque pale lilac
C0652 count von count transparent light purple
C0653 larkspur transparent pale purple
C0654 grape ape opaque medium purple
C0655 eggplant opaque dark purple
C0658 plum semi translucent light purple
C0660 crocus semi opaque light purple
C0661 evil queen opaque deep purple
C0667 poi opaque dark lilac
C0701 ginger opaque light pink
C0703 butter pecan opaque pale pink
C0717 khaki opaque gray green
C0722 canyon de chelly opaque light brown
C0742 sepia transparent pale pink
C0765 chai opaque pale pink
C0806 cirrus semi opaque white
C0820 hades opaque intense black
C0834 clear transparent clear
C0835 peace shimmering opaque white
C0859 marshmallow semi opaque white
C0904 gelly's sty opaque light pink
C0907 rose quartz semi opaque light pink
C0915 pink champagne translucent light pink
C0921 blush translucent pale pink
C0926 cranberry semi opaque rich dark pink
C0957 desert pink opaque pale pink


CiM Uniques

Further information

Visit their website for more information: http://www.creationismessy.com/