− | + | Designed for the [[glass worker]] with limited high pressure [[fuel]], this torch is intended to be highly efficient with its fuel whilst still being able to work with both [[soft glass]] and [[borosilicate]]. I has a 6 jet centre fire. | |
− | + | Full flame gas consumption: 5 cu. ft./hr (142 l/hr); [[oxygen]]: 12 cu. ft./hr. (341 l/hr) | |
+ | Will work rod upto 16mm and tube upto 19mm | ||
− | + | == Further information == | |
− | + | For more information see the [http://www.bethlehemburners.com/betta.htm The Bethlehem Betta Page] | |
− | |||
− |
Revision as of 13:28, 13 November 2008
Designed for the glass worker with limited high pressure fuel, this torch is intended to be highly efficient with its fuel whilst still being able to work with both soft glass and borosilicate. I has a 6 jet centre fire.
Full flame gas consumption: 5 cu. ft./hr (142 l/hr); oxygen: 12 cu. ft./hr. (341 l/hr)
Will work rod upto 16mm and tube upto 19mm