Revision as of 18:13, 13 November 2008 by Jolene(talk | contribs)(New page: Ask glass is currently out of production but is currently still available from a few stockists in a limited but bright colour palette. It is a brand of silver rich soft glass, compatible w...)
Ask glass is currently out of production but is currently still available from a few stockists in a limited but bright colour palette. It is a brand of silver rich soft glass, compatible with Effetre, Vetrofond and other CoE 104 Glass rods.