[[Ask]] [[glass]] is currently out of production but is currently still available from a few stockists in a limited but bright colour palette. It is a brand of silver rich [[soft glass]], compatible with [[Effetre]], [[Vetrofond]] and other [[CoE]] 104 Glass rods.
 