<?xml version="1.0"?>
<feed xmlns="http://www.w3.org/2005/Atom" xml:lang="en-GB">
	<id>https://www.frit-happens.co.uk/w/index.php?action=history&amp;feed=atom&amp;title=Removing_beads_from_mandrel</id>
	<title>Removing beads from mandrel - Revision history</title>
	<link rel="self" type="application/atom+xml" href="https://www.frit-happens.co.uk/w/index.php?action=history&amp;feed=atom&amp;title=Removing_beads_from_mandrel"/>
	<link rel="alternate" type="text/html" href="https://www.frit-happens.co.uk/w/index.php?title=Removing_beads_from_mandrel&amp;action=history"/>
	<updated>2026-11-20T03:21:51Z</updated>
	<subtitle>Revision history for this page on the wiki</subtitle>
	<generator>MediaWiki 1.45.1</generator>
	<entry>
		<id>https://www.frit-happens.co.uk/w/index.php?title=Removing_beads_from_mandrel&amp;diff=736&amp;oldid=prev</id>
		<title>Garishglobes: New page: Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can&#039;t remove them.  A: Soak in water, grip the rod with pliers close to the bead and gently twist th...</title>
		<link rel="alternate" type="text/html" href="https://www.frit-happens.co.uk/w/index.php?title=Removing_beads_from_mandrel&amp;diff=736&amp;oldid=prev"/>
		<updated>2010-09-24T12:08:12Z</updated>

		<summary type="html">&lt;p&gt;New page: Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can&amp;#039;t remove them.  A: Soak in water, grip the rod with pliers close to the bead and gently twist th...&lt;/p&gt;
&lt;p&gt;&lt;b&gt;New page&lt;/b&gt;&lt;/p&gt;&lt;div&gt;Q: I have made beads, with bead release on the mandrel, but now that they have cooled I can&amp;#039;t remove them.&lt;br /&gt;
&lt;br /&gt;
A: Soak in water, grip the rod with pliers close to the bead and gently twist the bead.&lt;br /&gt;
&lt;br /&gt;
Try putting them in the freezer for a short while, or soaking in Coke or Cillit Bang - this can help.&lt;/div&gt;</summary>
		<author><name>Garishglobes</name></author>