Main Menu

encased stringer?

Started by fionaess, January 30, 2008, 05:25:54 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

fionaess

Hi
How do I make an encased stringer please ???

Fiona


If it's got a hole, it's a bead !

turnedlight

You heat the clear/ transparent rod to very melty and swipe it down the other rod (warmed first) then keep it barely warm while melting another load to swipe down other side, then warm whole thing and pinch together the gaps with tweezers. then warm and pull like a stringer.. Clear? As mud I expect, I should leave it to the experts, but I have just done some of these today ;D
kathryn

Jolene

Hi Fiona

I just searched and found this on you tube
http://www.youtube.com/watch?v=vCatd0hSr_I

I will also add it to the tutorials section here.

Jo x

fionaess

Thank you both.... Im off to have a look at the vid and then have a go.. wish me luck as you wave me goodbye .. ;D

Fiona


If it's got a hole, it's a bead !

Stacy

is it just me or does anyone else reach for the diddys when you start to watch one of these DVDs to try to take the glare off, then have a DOH! moment when you realise of course it won't work!

Thats a great tut by the way... thanks jo!