Frit-Happens !
February 28, 2020, 03:46:31 PM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Re: Gaffer Chalcedony  (Read 615 times)
0 Members and 1 Guest are viewing this topic.
Tracy
Forum Member
*
Posts: 37



WWW
« on: July 01, 2009, 05:54:47 PM »

My first go.....considering it was five thirty this morning when I played, I am  quite chuffed!
Coarse frit pulled into stringer over eff light ivory opps  Roll Eyes

clickable!!
Logged

Veebee
Superglassyfrittylisticgirlmakes beadsatrocious!
Forum Member
****
Posts: 392


Serial HotHead on bulk user and glass murderess.


WWW
« Reply #1 on: July 07, 2009, 02:14:35 AM »

i cant get any pretty colours ;-(
i am ok with raku  but this one.... i have tried heating, got brown, tried striking, got brown, tried not heating, got brown !!
different bases too, have followed marys advice, but ..still brown  Roll Eyes
anyone got any tips??
s x

Same here! However, I heated the snot out of this one, did the gravity swirl thing then marvered to strike, and I got colour!
(**click on the image for a closer view**)



Try working it for a bit longer maybe?

I used CiM Khaki as a base.
Logged

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/
Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #2 on: July 07, 2009, 02:14:57 AM »

not the best picture - but I got this



I've also got one on black and one on white - but I need to take pics.

Sandy all I can say is what Mary said - sorry ......
Logged

sparrow
I hold with those who favor fire.
Senior Forum Member
*
Posts: 869


I'm working on a dream...


WWW
« Reply #3 on: July 07, 2009, 04:13:09 AM »

Right, I think I was overly polite......was the restriction one per size per person?? Or one per person, full stop? I went for the latter. If anybody ever makes jokes about Germans and towels or anything else, please remember this moment, lol!!

Anyways, you've seen him elsewhere, but he's Chalcedony on black, Size one:



Smiley
Logged

Diane
Forum Member
***
Posts: 233


WWW
« Reply #4 on: July 07, 2009, 08:13:29 AM »

Here's a shell set I've made using System96 (had it in for ages and only just using it Grin) glass and a mixture of No1 and No2 Chalcedony frits.:


Diane x
Logged

dinah46
Forum Member
****
Posts: 358



WWW
« Reply #5 on: August 02, 2009, 02:55:35 PM »

This is chalcedony stringer over silver foil, I'm beginning to really like this frit Cheesy



these are a mixture of small and chunkier frit


Logged

*rowanberry*
is just a figment of your twisted imagination
Forum Member
****
Posts: 433


quiet due to brain being replaced with fudge.


WWW
« Reply #6 on: August 14, 2009, 01:41:09 PM »

Wowzers Sam, they are fab!

Here's what I did with some stringers pulled from frit (cant wait to get hold of the cane!):




I found that chalcedony sometimes puts a dusky grey on ivory near where you put it. I liked it though as it made it look "old".
Logged

Claire
turnedlight
Forum Member
*****
Posts: 637

Kathryn


WWW
« Reply #7 on: August 18, 2009, 09:20:28 AM »

I got them out of the kiln, and I am chuffed with the results but they are a pig to photograph!
Here's the first, I heated and cooled several times, then I raked, and heated and cooled very gradually..
         
And here's the second
         

Love this glass! Smiley
Logged

kathryn
Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #8 on: September 02, 2009, 06:53:43 AM »

Here's a few from me - just had a quick play:



I'm really pleased with the colours - but not sure about the heart. The colours are great, but it's just so obvious where I had to add more glass ........ and doesn't blend in!
Logged