Author Topic: Meteorite glass  (Read 1109 times)
0 Members and 1 Guest are viewing this topic.
Marcel
Forum Member
****
Posts: 364


WWW
« on: April 19, 2017, 07:51:07 AM »

Here are two pendants i have made with glass produced by Guillaume Thoraval.
it is glass mixed with meteorite out of argentine. very special to work with







and this pendant i made using a Euro cent wich containes steel and copper so traces of it is blended with the clear glass

Logged
baked glass
New Forum Member
*
Posts: 19



WWW
« Reply #1 on: April 19, 2017, 10:02:27 AM »

I love that spirit bear. Nice work.

Is meteorite glass the same as tektite? I've been thinking it would be interesting to work with ever since I read an article about it in glassline.
 
Logged
Marcel
Forum Member
****
Posts: 364


WWW
« Reply #2 on: April 19, 2017, 10:28:23 AM »

Thank you Smiley no this is way different than tektite.
Tektite needs a lot of heat to melt! the meteorite glas is real soft and easy to melt.
here are two pendants i made of tektite first melted it not shape coldworked it and flamepolished after



Logged
baked glass
New Forum Member
*
Posts: 19



WWW
« Reply #3 on: April 21, 2017, 08:26:40 AM »

Great, thanks for that Marcel. Always nice to hear from someone who's actually worked with something rather than just read about it.