Frit-Happens !
June 13, 2021, 11:11:33 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Foodsafe Over glaze where is the best to get it in the uk.  (Read 3482 times)
0 Members and 1 Guest are viewing this topic.
Jules1971
New Forum Member
*
Posts: 11


« on: March 25, 2017, 10:21:37 AM »

Hi Guys where is the best place to buy in the Uk to by a foodsafe overglaze for bottle slumping.

Thanks all
Logged
Moira HFG
Half Full Glass
Forum Member
****
Posts: 416


Ever the optimist


« Reply #1 on: March 25, 2017, 01:04:24 PM »

I must admit I am stumped here, I didn't know you needed any sort of overglaze on a slumped bottle.  Huh
Logged

Jules1971
New Forum Member
*
Posts: 11


« Reply #2 on: March 26, 2017, 03:51:55 PM »

Hi moira it isnt so much that you need one i want to get a good glaze on some of my slumps especially if im going to use them for food.

Thanks Julian
Logged
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #3 on: March 29, 2017, 05:33:25 AM »

bullseye glass recommend a layer of clear over the coloured layer, but I don't know what you'd do when your base glass is of unknown coe
Logged
Moira HFG
Half Full Glass
Forum Member
****
Posts: 416


Ever the optimist


« Reply #4 on: March 29, 2017, 02:57:49 PM »

Yes, quite so. You might get away with a bit of frit to decorate the surface, up to 5%, but any more and it's likely to crack as it cools.
Most bottles that people slump were made for wine or other drinks, so should be fine to use for food.