Steampunkglass
Forum Member
*****
Posts: 736


Will work for Cat-food and Glass


WWW
« on: September 22, 2016, 01:49:03 PM »

Anybody made glass pens with glass nibs? The type where the nib is glass? I have a customer specifically asking for a special pen but with a glass nib.  Undecided Anyone got any tips to make them, contemporary glass has a paragraph on making them but not sure if anyone here has any practical experience of doing them and any tips?Huh
Logged

mel
Forum Member
***
Posts: 186


WWW
« Reply #1 on: September 22, 2016, 02:41:02 PM »

Sorry I cant be of any help whatsoever, but would be interested to hear of any progress you make!
Logged

Laughinglass Lampwork Beads
Moira HFG
Half Full Glass
Forum Member
****
Posts: 405


Ever the optimist


« Reply #2 on: September 22, 2016, 05:57:18 PM »

No - but there are a few things on Youtube....
Logged

Nicknack
Forum Member
****
Posts: 470

To bead, or not to bead? ..... stupid question!


« Reply #3 on: September 23, 2016, 01:50:44 AM »

I've seen Ray Skene do it, but it was several years ago. He was demoing. I would ask him if I were you.

Nick
Logged
tuffnell glass
Forum Member
***
Posts: 198



WWW
« Reply #4 on: September 23, 2016, 02:04:41 AM »

Hi,
   We used to make them but they would only hold enough ink for one or two short words .

Best wishes ,

Martin
Tuffnell Glass
Logged

baked glass
New Forum Member
*
Posts: 19



WWW
« Reply #5 on: September 28, 2016, 03:41:50 AM »

I've tried making the shape with a star mould and with laying down narrow stringers over a cone but have had not had total success with either.  They do write a bit, just don't hold the ink for very long.  There are some great tips at this site.  http://www.wetcanvas.com/forums/showthread.php?t=242948&highlight=glass+pens
Logged
Steampunkglass
Forum Member
*****
Posts: 736


Will work for Cat-food and Glass


WWW
« Reply #6 on: September 28, 2016, 03:45:50 AM »

Thank you all, I'll have a play around and see what I can do  Smiley
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.03 seconds with 19 queries.