Frit-Happens !
June 13, 2021, 09:42:20 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: paragon sc3  (Read 2535 times)
0 Members and 1 Guest are viewing this topic.
Shirl
Forum Member
****
Posts: 371


« on: December 15, 2015, 11:44:20 AM »

I finally got some time to make some beads and my kiln won't work, does anyone know where I can get a thermocouple?

Thanks in advance
Logged

Lee - Kilncare
Forum Member
****
Posts: 445


Kilncare annealing kilns. Designed by listening.


WWW
« Reply #1 on: December 15, 2015, 12:12:17 PM »

What makes you think you need a thermocouple?

Lee
Logged


TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732
Shirl
Forum Member
****
Posts: 371


« Reply #2 on: December 15, 2015, 02:08:05 PM »

Hi Lee, I am not so sure it is, but if it turns out to be faulty I would like to know where to get one.

I got the error tcl, thermocouple lag?
Logged

flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #3 on: December 15, 2015, 03:14:03 PM »

Hi
Do you have the manual? I've looked at the manual for my SC2 and there are several possible reasons.
1. worn or burned out elements, defective relays, low voltage and defective thermocouple
2. On kilns that use a portable controller, the thermocouple has fallen outside the firing chamber
3. a bare spot on the thermocouple lead wires has touched a grounded object inside the kiln causing the thermocouple to short out
4. you have programmed a cooling segment temperature that is below room temperature.

so I suppose the first one to check is number 4.
HTH, but it might not.
Logged
Shirl
Forum Member
****
Posts: 371


« Reply #4 on: December 15, 2015, 03:59:29 PM »

Yes l have the manual, and have eliminated some of the reasons for the problem.  It's not no.4, 3 or 2.

My son has tested it and seems to think it's low voltage and needs a new transformer, I hope he's right Smiley
Logged

Shirley
Forum Member
******
Posts: 830


WWW
« Reply #5 on: December 15, 2015, 05:43:21 PM »

The most common thing to go wrong is the relay. The tcl code doesn't really point to the thermocouple, in my experience.
Logged

Val Cox Frit - Thai and Bali Silver 
Shirl
Forum Member
****
Posts: 371


« Reply #6 on: December 16, 2015, 11:16:42 AM »

Thank you. I was going to replace the relay anyway, but my son seems to think it's the transformer.
He tried to buy one today but had no joy, does anyone know where l can get one?
Logged

Lee - Kilncare
Forum Member
****
Posts: 445


Kilncare annealing kilns. Designed by listening.


WWW
« Reply #7 on: December 16, 2015, 12:57:46 PM »

If it was the transformer, the chances are that the controller would not work at all.

My bet lies with the relay. Swap that, they aren't expensive but are the root cause of 90% of Paragon issues.
Logged


TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732
Shirl
Forum Member
****
Posts: 371


« Reply #8 on: December 16, 2015, 01:57:59 PM »

Thanks Lee, my son can get me a relay, so l will try that first.

Thanks again, I will update when l fix it.
Logged

chipperpottery
Life passes by when melting glass.
Forum Member
****
Posts: 370


WWW
« Reply #9 on: December 17, 2015, 03:37:58 AM »

ebay. I bought mine from.
Logged

Shirl
Forum Member
****
Posts: 371


« Reply #10 on: December 17, 2015, 04:25:31 AM »

Thanks for the info but hubby has ordered one through work, as they have an account with RS components and they sell them
Logged

Shirl
Forum Member
****
Posts: 371


« Reply #11 on: December 22, 2015, 05:28:43 PM »

I got a new relay and it's fitted, an easy job, all seems okay now. Many thanks to all for your help.