0 Members and 1 Guest are viewing this topic.
lemon kitten
Forum Member
***
Posts: 103



WWW
« on: October 10, 2015, 08:11:58 AM »

Can someone please advise how I can get a lovely sparkle effect using silver foil each time I roll it on the bead and then burn it off i do get sparkles but also it discolours the glass thanks folks!
Logged

Never stand up in a canoe!
Moira HFG
Half Full Glass
Forum Member
****
Posts: 390


Ever the optimist


« Reply #1 on: October 10, 2015, 10:52:20 AM »

Are you using colours that react with silver?
I don't know all the reacters, but the Bullseye chart is a help. Warm yellows, ambers and some greens react.

http://www.warm-glass.co.uk/images/pdfs/products/Reactive%20Glass%20Chart.pdf

Logged

Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #2 on: October 10, 2015, 04:49:50 PM »

I used to get this sometimes ... I thought  I was catchingit in the flame, someone else said  it was the temp of the flame ... it needs to be cooler.

Another way is to use palladium .... it is easierto works with and has a great shimmer.
Logged

lemon kitten
Forum Member
***
Posts: 103



WWW
« Reply #3 on: October 11, 2015, 05:20:46 AM »

Ahhhhh yeeees cooler flame....I'm using it over transparent blue and also over CIM Kryptonite  Will try that
Logged

Never stand up in a canoe!
Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.025 seconds with 18 queries.