Author Topic: foiled glass  (Read 997 times)
0 Members and 1 Guest are viewing this topic.
shafeenan
Forum Member
**
Posts: 77


« on: August 15, 2015, 05:00:04 PM »

Not sure I am in the right place, but....
I have some unusual shaped pieces of glass (offcuts from a glassblowing project) and want to use copper foil down just one side.
Can I safely do this if I go just round the corner, say, and maybe also add some wire wrapping and solder that into place to make sure the whole piece is held?
Also - can one use any kind of wire and will it take solder if you have cleaned it and used flux? thanks
Logged
Moira HFG
Half Full Glass
Forum Member
******
Posts: 830


Ever the optimist


« Reply #1 on: August 15, 2015, 06:52:17 PM »

This sounds like an interesting project!

I think you'll have to experiment - but remember that copper foil has no strength, it's the solder that provides that; also the gum on the foil strip is only strong enough to hold it in place whilst you do the solder work. You'll need to create a holder that will surround enough to glass to make it secure.

Copper wire is good for this sort of thing - soft, easy to manipulate, takes solder well (not coated wire, obvs!). I suppose steel wire might work if you have it, though rust might be a problem if you don't cover every bit with solder.
Logged

shafeenan
Forum Member
**
Posts: 77


« Reply #2 on: August 16, 2015, 10:44:27 AM »

thanks for your help - I'd not really grasped the basis of how the foil holds to the glass and you have clarified it in just a few words. I suppose one usually goes all the way round so it's not an issue.  Hopefully I will get something vaguely suitable and if so will post a picture so you can see what I've not been able to explain in words!  Fingers crossed.....!
Logged
Moira HFG
Half Full Glass
Forum Member
******
Posts: 830


Ever the optimist


« Reply #3 on: August 16, 2015, 01:11:08 PM »

I look forward to seeing what you come up with  Smiley

Here's something I did with foil and wire. This is dichro on black glass, so I could run foil all the way round without it looking too intrusive. With transparent glass it would look very different. Thinking about it, I'd probably have drilled a hole near the top to take the wire through to make it secure....there's an idea for you!)

Dichro earrings by Moira Robinson, on Flickr

 
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.033 seconds with 18 queries.