Colour testing DH frit on different bases

Started by paintboxcrafts, February 25, 2015, 02:36:53 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

paintboxcrafts


colour test by paintboxcrafts, on Flickr

I have been making some reference beads with DH frit over various bases, reduced an encased. I am not usually so organised!
From top to bottom the frits I used are Triton, Aion2, Ekho and Clio
From left to right the base colours are transparent purple, transparent striking orange, CIM Ghee, CIM Stoneground, Dark Ivory and Clear.

My favourites are the Clio on Ivory, Clio on trans orange, the Ekho on Ivory, and the Triton on Stoneground and Triton on trans orange.

Cathy
www.paintboxcrafts.co.uk  www.paintboxcrafts.etsy.com