anditsinthefish
Forum Member
***
Posts: 138



« on: January 14, 2015, 07:07:23 AM »

I have been thinking about a few ideas and wanted to try some drop melts however I only have a SC2... I have found some small pots to do the drop melts from and I would use kiln dams so I don't end up with a messy kiln.

Has anyone tried this?

Sarah xx
Logged

Sarah xx
Website. Blog. Flickr.
Pat from Canvey
Only a little bit odd
Forum Member
*******
Posts: 1222


Keep on blowing


« Reply #1 on: January 14, 2015, 08:30:17 AM »

Yes and I wouldn't recommend you try. I do my usual melts at 930 deg c in my big kiln and tried a tiny melt in my SC2. The amount of heat escaping through the bead door changed the blue paint colour to white even with a mass of ceramic fibre jammes accross the door to stop heat loss. The melt of Spectrum glass was fine though and about cabochon size.
Logged

anditsinthefish
Forum Member
***
Posts: 138



« Reply #2 on: January 14, 2015, 09:33:28 AM »

Yes and I wouldn't recommend you try. I do my usual melts at 930 deg c in my big kiln and tried a tiny melt in my SC2. The amount of heat escaping through the bead door changed the blue paint colour to white even with a mass of ceramic fibre jammes accross the door to stop heat loss. The melt of Spectrum glass was fine though and about cabochon size.

Thanks for the reply Pat... I suspected this might be the case. Fingers crossed for a premium bond win for a big girls kiln then. hmmm back to the drawing board.
Logged

Sarah xx
Website. Blog. Flickr.
GorgeousGlassGifts
New Forum Member
*
Posts: 22


« Reply #3 on: January 23, 2015, 04:51:11 PM »

Have you thought about hiring kiln time from one of the fusing glass suppliers near you, & doing a pot melt in their kiln? I don't know where you're based, but Creative Glass in Kent do kiln hire, as do Glass Studio Supplies, so your nearest supplier might too?
It might not be cheap, but it's got to be cheaper than buying a bigger kiln  Cheesy