Author Topic: Stiff oxygen knob on Nortel Minor  (Read 1497 times)
0 Members and 1 Guest are viewing this topic.
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 967


Just give me the coffee and no one gets hurt!


WWW
« on: October 29, 2014, 03:05:31 PM »

A new one on me, the oxygen knob on my Minor has got stiff, as if there is gunk in the thread that needs cleaning out.  I've undone it as far as it will go and cleaned with with a lint free cloth but still stiff.  My usual go-to is WD40 but not sure about using that on a torch.

Anyone any suggestions?  If I can't fix things with velcro, WH40 and blu tac then I get stumped!

Logged

Moira HFG
Half Full Glass
Forum Member
****
Posts: 384


Ever the optimist


« Reply #1 on: October 29, 2014, 05:21:19 PM »

No! Never use oil or grease in an oxygen line. I wonder if it's got cross-threaded somehow?
I'd take it to an engineering type bod to look at.
Logged

Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 967


Just give me the coffee and no one gets hurt!


WWW
« Reply #2 on: October 29, 2014, 05:27:01 PM »

Haven't any suitable engineering people around here and don't think it is cross threaded as it still works and isn't that stiff to be like a crossed thread.  I think it's just gunk from 3 years of general usage.  I'd rather not have to disassemble the torch (it's not leaking) as I don't have the ability to do this/reconnect and don't want to lug all the hoses and regulator around with me.  From experience with other things, even if I went into Bristol and could find anyone who would look at this (and I wouldn't know where to start in the phone book), they'd be likely to squirt it with something!
Logged

Moira HFG
Half Full Glass
Forum Member
****
Posts: 384


Ever the optimist


« Reply #3 on: October 29, 2014, 05:31:58 PM »

Can you see any gunk when you unscrew it?
Logged

Moira HFG
Half Full Glass
Forum Member
****
Posts: 384


Ever the optimist


« Reply #4 on: October 29, 2014, 05:38:01 PM »

If it's dust or grit in there, soapy water and cotton buds might shift it?
Logged

Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 967


Just give me the coffee and no one gets hurt!


WWW
« Reply #5 on: October 29, 2014, 05:47:23 PM »

Nope no gunk.  but I've just been down to my studio to check and it seems a bit freer, so perhaps I am just getting limp wristed in my old age.  Or you have telepathic super powers.  I'll see how it goes over the next few days.  Otherwise I'll try soapy water and a cotton bud, but was worried they might leave fluff?  Have already tacked with a small brush.  Thanks Smiley
Logged

the lady with the lamp
Forum Member
**
Posts: 61



« Reply #6 on: October 30, 2014, 08:10:39 PM »

What about using a small brush,old tooth brush or a small wire or nylon brush that might do it,Parin.