0 Members and 1 Guest are viewing this topic.
silkworm
Forum Member
**
Posts: 71


« on: September 21, 2014, 11:36:44 AM »

My ventilation suddenly began making a strange noise - loud, harsh rattle. It is a kit from Tuffnell's. I opened it up today and cannot see anything loose and am a bit reluctant to try to get in to the motor itself. Has anybody else had this happen?
Logged

Mary
Nicknack
Forum Member
****
Posts: 472

To bead, or not to bead? ..... stupid question!


« Reply #1 on: September 21, 2014, 11:57:13 AM »

Mine does it when it thinks the flame is a bit hot, and stops when I make it cooler.  I think I need to move the end nearest me a bit higher, so it's not so near the flame.

Nick
Logged
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #2 on: September 21, 2014, 12:25:16 PM »

My progrow fan did that when it got too hot.  I've got the box variety rather than the inline kind - in the end it fell apart on me once it stopped and cooled down Shocked Next time I'd go for the inline kind, I was told they don't usually fail?
Logged

Glyn Burton
Forum Member
***
Posts: 149


WWW
« Reply #3 on: September 22, 2014, 02:23:21 AM »

I had the same thing. The fans are made from a thermoplastic which soften and distort when they get hot causing them to rub against the casing and thus making the noise. In the end I bought a different fan and raised the inlet up a bit.