Cecilia
Forum Member
***
Posts: 114



WWW
« on: July 03, 2014, 05:30:43 AM »

Hi. I have had a request from a customer who would like a bead 1.5 - 2 inches, square, preferably flat and decorated with a pattern of medal ribbons. 8 ribbons to be precise.
I did suggest to her that it might be easier for a fuser to get the precise patterns, I am thinking tiny pieces of stringer to give the medal stripes.
I am quite happy if someone would like to take this over for me as I am not sure how I can do this.
I think it is a remembrance bead and it is important to her to get the pattern correct.
Any ideas.
Thanks. Cecilia X
Logged

Cecilia
Forum Member
***
Posts: 114



WWW
« Reply #1 on: July 04, 2014, 04:43:51 AM »

Help. X
Logged

Steampunkglass
Forum Member
*****
Posts: 736


Will work for Cat-food and Glass


WWW
« Reply #2 on: July 04, 2014, 05:00:56 AM »

Only thing I can think of is making a custom murine for the ribbons, then popping those onto the bead. It means a lot of work to make a murine that looks like a ribbon, but you'd have more control over the shape and colours, then once it's done you'll be able to make the bead fairly easily. Other way might be to look at decals, or paint them on?  Huh
Logged

Cecilia
Forum Member
***
Posts: 114



WWW
« Reply #3 on: July 04, 2014, 06:22:00 AM »

Hmmn tricky one. Thanks. X
Logged

marklaird
Forum Member
**
Posts: 90


WWW
« Reply #4 on: July 04, 2014, 06:22:53 AM »

Hi Cecilia,

I think I made something like this on a fusing course back in Jan. I've uploaded a photo to flickr.

https://flic.kr/p/ocjHz6    (for some reason I can't access the BBcode to link directly) but is this the sort of thing that you are after?

Mark
Logged

Fiona
Forum Member
***
Posts: 128


WWW
« Reply #5 on: July 04, 2014, 11:54:25 AM »

Do you have a picture of the pattern you need to produce?  That might make it easier for someone to suggest what you could do to achieve it.
Logged

Kaz
Flame Off Show Off
Senior Forum Member
*
Posts: 1251


Worth my weight in glass....


WWW
« Reply #6 on: July 04, 2014, 05:46:11 PM »

All I can say is...JUST SAY NO!!!
I think life's too short to spend it trying to meet other people's increasingly bizarre requests!
Logged

She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!
Flyingcheesetoastie
On Golden Wings of Cheddar...
Forum Member
****
Posts: 361


Mostly making glass...


WWW
« Reply #7 on: July 04, 2014, 06:28:56 PM »

Does it have to be a bead? If it's flat then this could easily be a glass kiln fired piece with the ribbons printed or painted on using enamels. Then a bail could be attached or holes drilled for hanging etc.

I get a lot of commissions and don't find anything too bizarre as long as it's something I know I can make and the client can afford to pay for.
Logged

Enchanted Cobwebs
Forum Member
****
Posts: 372


Housework is over rated


WWW
« Reply #8 on: July 05, 2014, 01:22:38 AM »

All I can say is...JUST SAY NO!!!
I think life's too short to spend it trying to meet other people's increasingly bizarre requests!


I agree! You may spend days trying to do it and then even if you produce something its 'not quite what I was after' or 'How much? its only a bead!' I have learned to say no if its not something I can do without thinking, I'd rather channel my workings out into something I am trying to create for my own satisfaction. My most recent NO was a teardrop pendant 70mm long just 5mm thick at one end and 30mm at the other
Logged

Now I can play all day as I retired from the 'proper' job....
http://www.enchantedcobwebs.com
http://www.etsy.com/shop/EnchantedCobwebs
Lakelady
TurnerRoweGlassArt
Forum Member
****
Posts: 357


Shakin that gl ass!


WWW
« Reply #9 on: July 05, 2014, 03:09:31 AM »

I agree you should just say no.  I do loads of commission work and if the client won't give me artistic license or asks for anything mm precise I won't do it.  It's safer and easier that way as people do tend to have unrealistic expectations!  Wink
Logged

Turner Rowe Glass Art
June
Forum Member
****
Posts: 271



« Reply #10 on: July 05, 2014, 04:28:01 AM »

All I can say is...JUST SAY NO!!!
I think life's too short to spend it trying to meet other people's increasingly bizarre requests!


Kaz has it spot on. I was once asked for a kite shaped bead with each quarter a different colour and I can't tell you how much time I spent for next to nothing and it was ok. Fusing sounds like a possibility but I don't have enough coloured stringers to try it myself.
Logged
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #11 on: July 08, 2014, 04:07:33 AM »

As you suggested, I think fusing would be best for this.
Logged
Flyingcheesetoastie
On Golden Wings of Cheddar...
Forum Member
****
Posts: 361


Mostly making glass...


WWW
« Reply #12 on: August 12, 2014, 04:12:17 PM »

Sometimes, it's nice to say Yes!  Wink









Logged

Corinne Lacy
Forum Member
*
Posts: 49


« Reply #13 on: August 12, 2014, 04:26:16 PM »

Wow!!! What a result!
Logged
Fiona
Forum Member
***
Posts: 128


WWW
« Reply #14 on: August 13, 2014, 02:53:39 AM »

That looks great Rachel. I bet she loves it.  Smiley
Logged