Hi,

Are there any other Effetre colours that are as soft (or very similar) as the Opaque white?

Failing that, and CIM that is a similar softness?


Thanks

Tony

www.beadables.co.uk

lampworklover

do you mean 'soft and easy to melt' or 'soft colour'? Being a bit dim here.

CIM Peace is a nice white to work with, and CIM Marshmallow is a semi-opaque white..

Hotglass28

Effettre Pea Green is nice and soft
www.facebook.com/pages/The-Owl-Goes-Hoot/567182803365298
www.etsy.com/uk/shop/TheOwlGoesHoot?ref=l2-shopheader-name

helbels

Effetre Ivory is very soft and Double Helix Zephyr is soft (if pricey!)

Tonyb

Quote from: lampworklover on June 23, 2014, 11:18:44 AM
do you mean 'soft and easy to melt' or 'soft colour'? Being a bit dim here.

CIM Peace is a nice white to work with, and CIM Marshmallow is a semi-opaque white..

Hi. I meant soft and easy to melt.

Thanks

Tony

www.beadables.co.uk

Shirley

Most Effetre opaques are soft, but white is probably the softest.