Sarah9959
Forum Member
**
Posts: 59


Oh for my hair to grow again


« on: April 23, 2014, 07:28:11 AM »

Hi

Question for George really but put here in case it interests anyone else.

I looked at stainless steel shot at Rio Grande and the price was good but postage came in at 30 for 3lb of shot.

Just wondered if you feel the better quality  is worth paying that amount of postage for?

I am aiming to produce beautifully shiny smooth silver findings and components for my own use [of course whether I will or not is another matter altogether]!!

Thanks again for your patience with my endless questions.

Sarah
Logged
mizgeorge
Administrator
*******
Posts: 817


Or should that be missus?


WWW
« Reply #1 on: April 23, 2014, 07:33:15 AM »

You need to contact them - they can ship USPS rather than the expensive rate - a friend just bought some and said it cost him about 22 in total (delivered).

Hope that helps!
Logged

Sarah9959
Forum Member
**
Posts: 59


Oh for my hair to grow again


« Reply #2 on: April 23, 2014, 08:45:01 AM »

Definitely helps - thanks  Smiley

Sarah
Logged
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #3 on: April 23, 2014, 05:38:33 PM »

I don't know anything about the differing qualities of shot, but I am using this and am happy with it
http://www.manchesterminerals.co.uk/acatalog/STAINLESS-STEEL-SHOT--1-Kg--94_089.html#SID=26

there's a good range of sizes in it, including tiny pointy bits to get into the nooks and crannies
Logged
Sarah9959
Forum Member
**
Posts: 59


Oh for my hair to grow again


« Reply #4 on: April 26, 2014, 04:14:04 AM »

Thanks for replies. Contacted Rio Grande who were very helpful and sorted out shot and postage so it is winging it's way to me right now Smiley