Forum Member
***
Posts: 102


note to self dog fur is highly flammible


WWW
« on: November 13, 2013, 05:12:29 PM »

hi my grandson came to visit and what with lolly being put down we kinda wasn't watching him properly and he messed about with the regulator knob on my propane tank
I cannt remember the exact setting it should be on
im using a hothead if that makes a difference
Logged

tish
Forum Member
***
Posts: 102


note to self dog fur is highly flammible


WWW
« Reply #1 on: November 14, 2013, 03:43:27 AM »

help please im talking about the knob thing that's not on the tank but on the hose next to the knob on the tap the one that can already set with the hose from tuffers please help
Logged

SilverGems89
Forum Member
****
Posts: 486

Hot Cheeks


« Reply #2 on: November 14, 2013, 04:19:01 AM »

Open it fully then turn back 1/4 to 1/2 a turn, it will be fine!
Logged

tish
Forum Member
***
Posts: 102


note to self dog fur is highly flammible


WWW
« Reply #3 on: November 14, 2013, 07:32:48 AM »

thats what I do for the one ON THE TANK  this one has numbers and is the other one not on the tank
Logged

Shirley
Forum Member
******
Posts: 831


WWW
« Reply #4 on: November 14, 2013, 07:49:25 AM »

Light the torch, see what happens. If the flame looks ok then it's fine. If not then adjust the regulator knob until it gives a good flame. Sorry, long time since I used my hothead Cheesy
Logged

Val Cox Frit - Thai and Bali Silver 
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #5 on: November 14, 2013, 08:05:13 AM »

could you post a photo?
Logged
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #6 on: November 14, 2013, 12:00:23 PM »

The knob on the top of the tank should be full on so in an emergency there is only one way to go.

The big one with numbers that is near the screw in bit to the tank, the regulator, as Gems says, turn full on and then back a bit.
Logged

SilverGems89
Forum Member
****
Posts: 486

Hot Cheeks


« Reply #7 on: November 14, 2013, 03:07:01 PM »

What Sue said  Grin
Logged

tish
Forum Member
***
Posts: 102


note to self dog fur is highly flammible


WWW
« Reply #8 on: November 14, 2013, 05:22:44 PM »

ok thankyou everyone
Logged