catriona
Forum Member
***
Posts: 117



« on: August 15, 2013, 08:11:30 AM »

Hi can i pick you dear lady,s brains o have a 600mm wide work top and a Tuffnels vent kit.
My question is how far is the min distance that the torch can be to the cone.
  thanks in advance.
XXcatxx
Logged
Madam Steph
Forum Member
****
Posts: 440


Jon Snow just CAN'T be dead!


WWW
« Reply #1 on: August 15, 2013, 08:35:21 AM »

I'm not sure on dimensions, Cat, but I have worked with mine like this for 3 years now:



You can see my Cricket is quite close to the trumpet but it never burns it

Linda x
Logged

helbels
Proudly achieving mediocrity since Sept 2009.
Forum Member
******
Posts: 890


WWW
« Reply #2 on: August 15, 2013, 10:39:51 AM »

Try the smoke test.. Light a match or joss stick, and hold it at the head of your torch with the ventilation running.  If the smoke gets sucked up by the ventilation then it's close enough... if it doesn't, then move the ventilation closer until it does.
Logged

catriona
Forum Member
***
Posts: 117



« Reply #3 on: August 15, 2013, 10:48:06 AM »

Thank,s guy,s got it placed now my worrie was it was going to be too close but it,s ok.
xxcatxx
Logged
Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.03 seconds with 20 queries.