Started by Trudi, February 08, 2013, 08:48:43 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Trudi

Hi

Is is possible to fuse a wire hook onto a single 3mm piece of glass - I tried it last night but the wire - nichrome came away.

Thanks x

Zeldazog

Only by sandwiching it, Trudi - nothing really fuses to glass, other than glass (enamels are actually glass, decals are printed with ceramic or glass pigments, which contain glass...

You could put a small strip just where you want to add the wire, as opposed to over the whole piece (IYGWIM?)