soldering torch recommendations?

Started by marijane, April 12, 2013, 12:28:03 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.


mizgeorge

Smiths Little Torch (or similar - Hoke, Swiss etc). You need to keep the oxygen flow VERY low - under 2lpm and dial it in very carefully or it will blow the flame out. You can't use the smallest (ruby) tips with an oxypropane setup, but the others, including casting tips, work perfectly.